dianadvash Posted February 6, 2013 Report Share Posted February 6, 2013 hi, I have fired mistakenly the bisque on 1200. How do i glaze? Thank you, Diana Link to comment Share on other sites More sharing options...
Lucille Oka Posted February 6, 2013 Report Share Posted February 6, 2013 1200 what centigrade or Fahrenheit? Link to comment Share on other sites More sharing options...
Marcia Selsor Posted February 6, 2013 Report Share Posted February 6, 2013 1200 C would be about ^5. You may have vitrified the clay body depending on the type of clay you are using. Some glazes may still cling to the surface. You can try heating the pots before trying to glaze. You can try adding a little gum to the glaze and spray it on.. Marcia Link to comment Share on other sites More sharing options...