druttaro    0

I am making a bowl and want to apply glaze at cone 10 only on the inner surface, then refire it at cone 5 with underglaze for vibrant colors. Is this even possible? Will the inner glaze be damaged? Any help is welcomed!

Share this post


Link to post
Share on other sites
Marcia Selsor    1,301

Yes it is possible but be careful that you don't shock the matured/vitrified clay on the second glaze firing. you may have a tricky time getting the ^5 glaze to stick after the ^10 firing but it is possible. You can get brighter colors at ^10 if you use encapsulated stains. That could save you the hassle of 2 glaze firings and struggling with glaze application on a vitrified body.

 

 

 

Marcia

Share this post


Link to post
Share on other sites
druttaro    0

Thanks for the replies.

 

I do have a test piece drying but wanted to see if it was even possible. I am not to concerned with color change to the ^10 glaze but don't want it to change texture.

 

I am doing sugar skulls so will be happiest with good color on the outside.

post-21991-136009281111_thumb.png

post-21991-136009281111_thumb.png

Share this post


Link to post
Share on other sites
bciskepottery    925

Something to think about . . . why not use a cone 5/6 claybody, glaze fire to cone 6 and apply the underglazes for the same fire? I am assuming your underglazes are for the sprigs attached to the outside of the bowl. Save yourself time and the cost of the extra firing.

 

 

Share this post


Link to post
Share on other sites
Mark C.    1,807

I am a cone guy-and most glazes will change somewhat when fired again to lower temp. That is a shiny glaze can become matt etc.

I am with Marcia on the cone 6 all the way body-

Testing is the only way to know any of this as you are in unchartered territory.

Mark

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×