Jump to content

preparing raw majolica glaze for surface decoration.


Babs

Recommended Posts

Hi I am looking for a way to make my raw majolica glaze "harder" so that I can ddo more painterly desings on my ware. Mybrush tends to clog up with the glaze powder and so the lines are interrupted.

Hope somepone can help. I think I readd somewhere that you can spray something onto the glaze.Does any one have any hints.

Babs

Link to comment
Share on other sites

  • 2 weeks later...

add CMC to your base glaze. commercial glazes contain a good amount of this in their recipe. it forms sort of a "candy coating" and stiffens up the unfired glaze, which will be more resistant to your detail brush. start with around 1% or keep a thick solution of it in a jug to add to your glazes, underglazes, and stains/washes.