Hello

I want to know if there is a kind of ceramic offset lithography ink that can print ceramic decals by offset machine instead of current methods?

Now there is two methods that you can see below. http://en.wikipedia.org/wiki/Ceramic_decal

1-silk screen printing

2- lothography printing

but in my point of view in litho printing still there is no ink that can print directly like screen printing and now

with ceramic litho prints. instead of using ceramic inks. litho varnish is used for each colour. After passing through the litho press. the decal paper is dusted with pigment ...

 

can anyone give me some information in which a company had invented this ink before and if not can it be used in industry? or it is a Wild-goose chase and zero scoring effort and it is better i dont wast my time on this ?

Share this post


Link to post
Share on other sites

They now make inkjet printers that print decals. Don't know if this will help you at all, but it may be worth looking into.

 

Thank you neilestrick

 

can you please give me more information ? any video , photo or website ..?

I think inkjet printers are slow but offset machine is so fast and economical , there is no machine that can compete with it.

Share this post


Link to post
Share on other sites

Farzad,

If you're looking for commercial grade solutions to a manufacturing question, chances are you're barking up the wrong tree. A ceramic engineer might be the person to talk to, or someone with a materials science background with an emphasis in ceramics. Most of us here are potters who are not working on the scale or with the equipment you're talking about and can probably offer you information that is speculative and incomplete at best.

 

Good Luck,

Michael

Farzad likes this

Share this post


Link to post
Share on other sites

Farzad,

If you're looking for commercial grade solutions to a manufacturing question, chances are you're barking up the wrong tree. A ceramic engineer might be the person to talk to, or someone with a materials science background with an emphasis in ceramics. Most of us here are potters who are not working on the scale or with the equipment you're talking about and can probably offer you information that is speculative and incomplete at best.

 

Good Luck,

Michael

 

 

Thank you michael

my problem is that i dont know any engineer or anybody that work in this field

those who know about offset machine and printing media dont know about ceramic industry

and those who know about ceramic dont know about offset printing.

 

 

 

Share this post


Link to post
Share on other sites

Hello

I want to know if there is a kind of ceramic offset lithography ink that can print ceramic decals by offset machine instead of current methods?

 

That is an interesting question. I would ask Atlas Ink in Dallas, Texas if they could make an offset ink that could print ceramic decals. Atlas is a very good ink company. We use that ink for the Paragon catalog and manuals.

 

Sincerely,

 

Arnold Howard

Paragon Industries, L.P., Mesquite, Texas USA

ahoward@paragonweb.com / www.paragonweb.com

Farzad likes this

Share this post


Link to post
Share on other sites

My question is after you print 15,000 litho decals per hour then what-can you fire 15,000 decals per hour-lets say an 8 hour day with 120,000. decals.

What is the end use of decals to be fired on in mass amounts?

Mark

Farzad likes this

Share this post


Link to post
Share on other sites

Hello

I want to know if there is a kind of ceramic offset lithography ink that can print ceramic decals by offset machine instead of current methods?

 

That is an interesting question. I would ask Atlas Ink in Dallas, Texas if they could make an offset ink that could print ceramic decals. Atlas is a very good ink company. We use that ink for the Paragon catalog and manuals.

 

Sincerely,

 

Arnold Howard

Paragon Industries, L.P., Mesquite, Texas USA

ahoward@paragonweb.com / www.paragonweb.com

 

 

Thank you Arnold I am waiting for your news ,

 

 

 

Share this post


Link to post
Share on other sites
Thank you Arnold I am waiting for your news ,

 

I wasn't clear. Sorry. I meant that if I were you, I would ask Atlas Ink. You can contact them on their website. They are very knowledgeable. They may have already produced ceramic decal ink or know if it is feasible. Silk screening can lay down a much thicker layer of ink than is possible with offset printing. Bumper stickers are generally printed by silk screen, because the thicker the layer of ink, the longer it tends to last in sunlight. A thick layer of silk screen ink would probably also fire better than a thin layer of offset ink.

 

Sincerely,

 

Arnold Howard

Paragon Industries, L.P., Mesquite, Texas USA

ahoward@paragonweb.com / www.paragonweb.com

Farzad likes this

Share this post


Link to post
Share on other sites

My question is after you print 15,000 litho decals per hour then what-can you fire 15,000 decals per hour-lets say an 8 hour day with 120,000. decals.

What is the end use of decals to be fired on in mass amounts?

Mark

 

 

 

we will sale it to big ware factories !

No need to produce 15000 pcs decal papers ,with this method we can produce the same amount in 1 hour,while it takes 4 days with silk screen.

this method increases the speed specially in mass production so can reduce the costs too.

Share this post


Link to post
Share on other sites
Thank you Arnold I am waiting for your news ,

 

I wasn't clear. Sorry. I meant that if I were you, I would ask Atlas Ink. You can contact them on their website. They are very knowledgeable. They may have already produced ceramic decal ink or know if it is feasible. Silk screening can lay down a much thicker layer of ink than is possible with offset printing. Bumper stickers are generally printed by silk screen, because the thicker the layer of ink, the longer it tends to last in sunlight. A thick layer of silk screen ink would probably also fire better than a thin layer of offset ink.

 

Sincerely,

 

Arnold Howard

Paragon Industries, L.P., Mesquite, Texas USA

ahoward@paragonweb.com / www.paragonweb.com

 

Offset machine has a better quality , and for thickness we will print each colour several times and for drying we will use UV resin ,

 

 

can you please send me their page address ?

 

 

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.