I can't find any recipes for a cone 6 "color active," or fluxing slip. I'm really not sure what designates a slip as such, beyond the presence of more than normal percentages of flux(s). If I were to use a lower cone slip would it act like a color active slip?

 

Joel.

Share this post


Link to post
Share on other sites

Colored slips for me are slip (made from whatever clay body I choose) with added colorants to get a colored slip.-Fluxing slips for me are slips with fluxes added or lower cone clays which flux at high temps-I never have used ether .

I have colored porc or stoneware to make colored slips-most of this has been salt fired.

I have no idea what a color active slip is?

Mark

Share this post


Link to post
Share on other sites

I'm not totally sure, but i think if you added like one part frit 3124 to one part colored slip you'd have a color active slip.

 

 

 

Darrel

 

 

Thanks Darrel, I'll try a test using 3124.

 

I'm not sure either Mark. For now it is a pottery term that is awaiting concise definition. Like so many other pottery terms, it may never find one, heh.

 

Joel.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.