I can't find any recipes for a cone 6 "color active," or fluxing slip. I'm really not sure what designates a slip as such, beyond the presence of more than normal percentages of flux(s). If I were to use a lower cone slip would it act like a color active slip?

Joel.

#2 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,412 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 21 January 2013 - 01:32 PM

Colored slips for me are slip (made from whatever clay body I choose) with added colorants to get a colored slip.-Fluxing slips for me are slips with fluxes added or lower cone clays which flux at high temps-I never have used ether .
I have colored porc or stoneware to make colored slips-most of this has been salt fired.
I have no idea what a color active slip is?
Mark
Mark Cortright
www.liscomhillpottery.com

#3 Iforgot

Iforgot

    Advanced Member

  • Members
  • PipPipPip
  • 155 posts
  • LocationColorado

Posted 21 January 2013 - 11:05 PM

I'm not totally sure, but i think if you added like one part frit 3124 to one part colored slip you'd have a color active slip.



Darrel
Derek VonDrehle

Raku, Pit fired, Majolica, and Stoneware ceramic artisit

#4 yedrow

yedrow

    Advanced Member

  • Members
  • PipPipPip
  • 405 posts

Posted 21 January 2013 - 11:18 PM

I'm not totally sure, but i think if you added like one part frit 3124 to one part colored slip you'd have a color active slip.



Darrel


Thanks Darrel, I'll try a test using 3124.

I'm not sure either Mark. For now it is a pottery term that is awaiting concise definition. Like so many other pottery terms, it may never find one, heh.