I've been saving my throwing scraps and slip in a bucket with the intent of making a dipping slip (occasionally I'll use a hand blender to smooth it out). I use Highwater Little Loafers fired to cone 5 and was told the easiest way to make slip was to just use the clay body you throw with. The part I'm trying to figure out now is how to color the slip so that it fires black and looks black when covered with a clear glaze. I read on some forums that using Mason Stains could work. Has anyone used Mason Stains before to make a color dipping slip? If so, what is a good ratio to start testing out with?

Also, any suggestions on which one black stain to pick (http://www.sheffield...tains-s/106.htm) based on non-toxicity and/or behavior? Still learning the chemistry side of colorants and glazes so any tips are appreciated.

#2 bciskepottery

bciskepottery

    Advanced Member

  • Moderators
  • 2,703 posts
  • LocationNorthern Virginia

Posted 20 January 2013 - 09:37 AM

You might want to start out with a ratio of 10% mason stain to the amount of dry Little Loafers; 6600 black is a good one to start with. Also consider doing a progession test . . . 2%, 5%, 7%. 10% to see how it affects colors. The key will be to sieve the stain and slip to make sure it is well blended.

Different mason stains need different amounts in slip . . . but at some point you will reach a saturation point where adding more stain does not affect the color result. So, some experimentation is encouraged. No need to add more stain (and dollars) than needed.





#3 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,116 posts
  • LocationRaleigh, NC

Posted 20 January 2013 - 12:14 PM

I agree with the answer above but would add that the glaze you put over it could change the color so test them too. I use Amaco zinc free clear and seem to get true colors.
Chris Campbell Pottery
Contemporary Fine Colored Porcelain
http://ccpottery.com/

>TRY ... FAIL ... LEARN ... REPEAT"

" If a sufficient number of people are different, no one has to be normal "

Fredrick Bachman




0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users