georgio

Fusing Art To Ceramic

Recommended Posts

I am trying to transfer my work to ceramic and I am using laser paper and a laser printer but when I put it in the kiln it all burns off,,,could it be that I am using the wrong toner cartridge in my printer ..please i need help

Share this post


Link to post
Share on other sites

Paul Andrew Wandless would be a great person to help you. He is the King of printing on clay! If you can, get a hold of his book to cover some of the technical aspects of the successfully printed image. You may be able to buy it with a discount through here if you are a member. Also on Amazon: Paul's book

 

I know the key is the iron in the printing ink. Also, how are you firing?

Share this post


Link to post
Share on other sites

Paul Andrew Wandless would be a great person to help you. He is the King of printing on clay! If you can, get a hold of his book to cover some of the technical aspects of the successfully printed image. You may be able to buy it with a discount through here if you are a member. Also on Amazon: Paul's book

 

I know the key is the iron in the printing ink. Also, how are you firing?

 

 

Great response. Iron is the key and I believe HP printers have the toners?

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×