Posted 16 January 2013 - 03:57 PM

How do you convert US glaze recipes to something usable in EU?
I have few really nice high fire glaze recipes, I like to try out, but they are mostly made of US materials so almost useless in EU.
I also bought a wonderful book called "The Complete Guide to High-Fire Glazes, Glazing & Firing at Cone 10" but this is also US specific (btw, thank you for the Kg, g and °C Posted Image

Has anyone made a conversion table for converting those materials to stuff available in EU?

Or even better, can you point me to a active English (non US!) ceramics forum? I am usually OK finding stuff with google but in those 2 tasks I have failed Posted Image

Cheers!

#2 ayjay

ayjay

    Advanced Member

  • Members
  • PipPipPip
  • 485 posts
  • LocationHampshire, UK.

Posted 16 January 2013 - 04:43 PM

Or even better, can you point me to a active English (non US!) ceramics forum?


I've looked too; and whilst I've found a couple of UK based pottery forums they are not very active.

Emmanuel Cooper lists a few UK/US alternatives in the back of his book (The Potters book of Glaze Recipes), I'm sure others do too, if you put a list of ingredients on here I'm sure someone could help translate/convert at least some of them.

#3 SShirley

SShirley

    Cow Creek Pottery

  • Members
  • PipPipPip
  • 199 posts
  • LocationPittsburg, Kansas

Posted 16 January 2013 - 04:53 PM

You might try to contact Alisa Clausen in Denmark. She often lists US recipes and then substitutes European materials.
http://www.flickr.co...[email protected]

#4 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,146 posts
  • LocationRed Lodge, Montana

Posted 16 January 2013 - 04:53 PM

Michael Bailey's Glazes Cone 6 has UK and American Chemicals listed with their compositions.
Mastering Cone 6 Glazes by Ron Roy and John Hesselberth list compositions of US and Canadian firts and compositions of of materials. I do not think these refer to anything in Europe.

Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#5 macdoodle

macdoodle

    Advanced Member

  • Members
  • PipPipPip
  • 84 posts
  • LocationOrange County, CA, USA

Posted 16 January 2013 - 06:53 PM

will this be a good start? http://www.kentpotte...b/glaze_db.html

for temps its easy to convert - here is one site- http://www.albireo.c...atureconverter/

#6 Brian Reed

Brian Reed

    Advanced Member

  • Members
  • PipPipPip
  • 219 posts
  • LocationWashington State

Posted 16 January 2013 - 06:58 PM

I did not even think about the lack of the same materials in the EU because many of the published glaze recipes are made in the US. However I think the best source would be a program like Digital Fires Insight where you can look at the material list and see the mineral breakdown of each material and then can make a substitution for something local. This should allow you to make a very close glaze and not add or delete vital minerals or oxides that are needed.

Of course you could do this all manually by going to each manufacturer and getting the atomic weight of each element and then find a local supplier that will find a substitute item that closely resembles your item.

However this does not take the place of testing. You must test every material used in glaze as well as the clay body you are using. Test test test.



My 2 cents.
Brian Reed

Throwing down in Washington State

http://www.reedpottery.com

Northwest Clay Club

#7 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 4,828 posts
  • LocationGrayslake, IL

Posted 17 January 2013 - 10:34 AM

Glaze calculation software will allow you to make a recipe from the Unity Molecular Formula of a glaze, using the materials available to you. I substitute ingredients in recipes all the time this way because I keep a limited supply of glaze materials in my inventory. This is a great way to learn about glaze formulation, and you will be able to create a glaze that is nearly identical to the original. I have used Hyperglaze for many years, but there are other good glaze calc programs out there, too.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]


#8 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,131 posts
  • LocationWilton, NH USA

Posted 19 January 2013 - 11:56 AM

The trick for most of this (glaze wet batch rheology aside) is to use FORMULAS not recipes. Formulas can cross raw material sourcing to a large degree.

Molecular glaze calculation is the route to go to understand this. I recommend Digitalfire's "Insight" program. It is what I use in my college ceramic materials courses (and have since it was a DOS version!).

best,


...........john

John Baymore
Professor of Ceramics; New Hampshire Insitute of Art

Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#9 Mart

Mart

    Advanced Member

  • Members
  • PipPipPip
  • 283 posts

Posted 19 January 2013 - 05:11 PM

Thank you for all the replies.
http://digitalfire.c...sight/index.php looks interesting. Nice, they have Linux version available too.

alisaclausen has some cool stuff. Thank you. I have to look around there, maybe she has some cone 9 recipes because the works-shop I go, never fires below cone 9.

Thank you