Posted 14 January 2013 - 11:20 PM

Okay, it isn't earth shattering, but it seems to be a decent glaze. I think I need to flux it a little more to get what I want.

Posted Image

#2 Brian Reed

Brian Reed

    Advanced Member

  • Members
  • PipPipPip
  • 219 posts
  • LocationWashington State

Posted 14 January 2013 - 11:55 PM

Nice I like the transparent breaking on the rim.
Brian Reed

Throwing down in Washington State

http://www.reedpottery.com

Northwest Clay Club

#3 SmartsyArtsy

SmartsyArtsy

    Chris Seminara

  • Members
  • PipPipPip
  • 182 posts
  • LocationPNW

Posted 15 January 2013 - 12:25 AM

Very nice, yedrow. I like the depth. Do you have rutile or ilmenite in it?

#4 Hermes

Hermes

    Member

  • Members
  • PipPip
  • 16 posts
  • LocationHolsbeek, Belgium.

Posted 15 January 2013 - 04:11 AM

Okay, it isn't earth shattering, but it seems to be a decent glaze. I think I need to flux it a little more to get what I want.

Posted Image


I think this is a more than decent glaze.

Hermes

#5 atanzey

atanzey

    -

  • Members
  • PipPipPip
  • 147 posts
  • LocationSouth-Central Pennsylvania

Posted 15 January 2013 - 06:22 AM

I LIKE it! You may inspire me to try my own formulations! (With the help of a program, of course). Are you going to be interested in sharing? ;-)

Alice

#6 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,326 posts
  • LocationRed Lodge, Montana

Posted 15 January 2013 - 06:34 AM

I like the surface. The color is not for me , but it is a nice surface and breaking color change.
Very decent indeed!!!
Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#7 minspargal

minspargal

    Advanced Member

  • Members
  • PipPipPip
  • 90 posts
  • LocationPort Aransas, Tx

Posted 15 January 2013 - 08:52 AM

Oh very nice glaze, reminds me of the rutile blue glaze we used to use at school.

#8 TJR

TJR

    Advanced Member

  • Members
  • PipPipPip
  • 1,821 posts
  • LocationWinnipeg,Manitoba,Canada

Posted 15 January 2013 - 09:06 AM

yedrow;
What is it you are trying to achieve? If you fluxed it more, it will run more. I like the colour and surface. Keep going!
TJR.

#9 yedrow

yedrow

    Advanced Member

  • Members
  • PipPipPip
  • 405 posts

Posted 15 January 2013 - 10:11 AM

Thank you Brian!
Thank you Chris, it has rutile in it.
Thank you Hermes, you helped!!!

Thank you Alice, I'm going to share some, but as I put my pallet together I'll probably get a little stingy, at least for a couple of years. I'm not very good at being stingy though.
Thank you Marcia!
Thank you minspargal, good eye.
TJR, it has some dry spots in the glaze that I think would come out if it were fluxed better or fired longer. However, I'm pushing the body at present so I'm thinking I need to go the more fluxing route.

I'm really digging this glaze stuff. I've been working hard the last year to understand glazes and their chemistry. With Hermes help I got a much better understanding, and the Britt video really helped me in adjusting application. And being on this board with all the great talent and knowledge, and with those like me who are developing potters, has helped a great deal.

Thanks all,

Joel.