Does anyone know where you can buy pentalite in the USA.

Larry

Lawrence Weathers

Gismo Guy

Spokane WA


#2 perkolator

perkolator

    Advanced Member

  • Members
  • PipPipPip
  • 454 posts
  • LocationCalifornia

Posted 09 January 2013 - 07:11 PM

pentalite, or did you mean petalite? i've never heard of pentalite, but if you meant' petalite; any ceramics supplier or industrial minerals should be able to help you. usually runs around $2.5/lb

#3 docweathers

docweathers

    Gismo Guy

  • Members
  • PipPipPip
  • 643 posts
  • LocationSpokane Wa

Posted 09 January 2013 - 07:51 PM

Thank you for the correction in spelling. That's the reason I couldn't find it anywhere. I now have it on , thanks to your clarification.

Larry

Lawrence Weathers

Gismo Guy

Spokane WA


#4 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,310 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 10 January 2013 - 11:51 AM

petalite as used in Rietz green is available where fine glaze materials are sold.