Good morning everyone,

 

I'm a newbie to ceramic tile making and have a question. I broke one of my tiles in a mosaic and it is in the bone-dry state and underglazed. Is it possible to rejoin these two pieces with a slip made from the same clay body, or do I have to recarve the one tile? Thanks for any insight into this. Eddie

Share this post


Link to post
Share on other sites
Marcia Selsor    1,301

Mix up some patch with toilet paper and your slip. dampen both sides and join together. I have also patch bisque this was as well. It takes more dampening on bisque. Put the toilet paper in water overnight. Then in a blender with a drier version of your slip so the water in the TP doesn't make the solution thinner than desired. You want a paste/slip consistency.

Share this post


Link to post
Share on other sites
Dinah    6

This works for me. Using a mortar and pestle, pulverize some of the clay body you've used for the tiles. Add vinegar -- white/cider -- until you've got slip consistency. Take a spray bottle and carefully dampen both edges of the pieces to be repaired or dab edges with a brush. Then brush on the paste, marry up the edges and smooth and so forth. Wrap piece up until it's "cured" -- overnight.

Share this post


Link to post
Share on other sites
Chris Campbell    1,088

It also depends on how forgiving your clay body is.

 

If neither of those two replies work, then wrap the tile in a wrung out to just damp towel, then

wrap it in dry cleaner plastic and leave overnight. You want to add just a bit of dampness to

the entire tile but you don't want to wet it.

 

Then try either of the previous solutions again.

Share this post


Link to post
Share on other sites
EASloan    0

Thank you all for the quick replys. I will be trying these possible remedies before the week is out. I have the mural I'm doing sitting for a couple months now in the bone-dry state, and I broke this same tile twice already. I'm tired of making it, so hopefully one of the techniques you've provided will work for me. Being new to tile making, I now understand the beauty of making molds! Thanks again. I'll post pictures of some of my work I just fired. Eddie

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×