Good morning everyone,

I'm a newbie to ceramic tile making and have a question. I broke one of my tiles in a mosaic and it is in the bone-dry state and underglazed. Is it possible to rejoin these two pieces with a slip made from the same clay body, or do I have to recarve the one tile? Thanks for any insight into this. Eddie

#2 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,207 posts
  • LocationRed Lodge, Montana

Posted 27 July 2010 - 08:20 AM

Mix up some patch with toilet paper and your slip. dampen both sides and join together. I have also patch bisque this was as well. It takes more dampening on bisque. Put the toilet paper in water overnight. Then in a blender with a drier version of your slip so the water in the TP doesn't make the solution thinner than desired. You want a paste/slip consistency.
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#3 Dinah

Dinah

    Advanced Member

  • Members
  • PipPipPip
  • 178 posts
  • LocationNorth of Seattle, WA.

Posted 27 July 2010 - 10:04 AM

This works for me. Using a mortar and pestle, pulverize some of the clay body you've used for the tiles. Add vinegar -- white/cider -- until you've got slip consistency. Take a spray bottle and carefully dampen both edges of the pieces to be repaired or dab edges with a brush. Then brush on the paste, marry up the edges and smooth and so forth. Wrap piece up until it's "cured" -- overnight.
Dinah
www.DinahSnipesSteveni.com

#4 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,089 posts
  • LocationRaleigh, NC

Posted 27 July 2010 - 03:18 PM

It also depends on how forgiving your clay body is.

If neither of those two replies work, then wrap the tile in a wrung out to just damp towel, then
wrap it in dry cleaner plastic and leave overnight. You want to add just a bit of dampness to
the entire tile but you don't want to wet it.

Then try either of the previous solutions again.
Chris Campbell Pottery
Contemporary Fine Colored Porcelain
http://ccpottery.com/

>TRY ... FAIL ... LEARN ... REPEAT"

" If a sufficient number of people are different, no one has to be normal "

Fredrick Bachman

#5 EASloan

EASloan

    Newbie

  • Members
  • Pip
  • 5 posts

Posted 27 July 2010 - 08:14 PM

Thank you all for the quick replys. I will be trying these possible remedies before the week is out. I have the mural I'm doing sitting for a couple months now in the bone-dry state, and I broke this same tile twice already. I'm tired of making it, so hopefully one of the techniques you've provided will work for me. Being new to tile making, I now understand the beauty of making molds! Thanks again. I'll post pictures of some of my work I just fired. Eddie