I saw in a youtube video a guy using a plastic knife for shaping.
When I trim the top off of a pot I have difficulty using the long needle tool because of its lack of support, I use a thumb tack and get it right every time (the point is not too short because I tend to pull too thin rather than too thick)

What random objects have you used for tools and for what purpose?


~ Namaste ~

 

Home studio potter 

 

Shanel Pottery 

www.shanelpottery.com

www.facebook.com/shanelspottery 

 

 

 

"To me the greatest thing is to live beauty in our daily life and to crowd every moment with things of beauty.  It is then, and then only that  the art of the people as a whole is endowed with it's richest significance.  For it's products are those made by great a many craftsmen for the mass of the people, and the moment this art declines the life of the nation  is removed far away from beauty.  So long as beauty abides in only in a few articles created by a few geniuses, the kingdom of beauty is nowhere near realization."                                                                                 - Bernard Leach 

#2 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,116 posts
  • LocationRed Lodge, Montana

Posted 04 January 2013 - 12:52 PM

There was a long thread on a similar topic called " the proper inappropriate use of tools."

http://ceramicartsda...__fromsearch__1

Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#3 Rebekah Krieger

Rebekah Krieger

    The extraordinary clay bender

  • Members
  • PipPipPip
  • 786 posts
  • LocationWisconsin

Posted 05 January 2013 - 01:09 AM

There was a long thread on a similar topic called " the proper inappropriate use of tools."

http://ceramicartsda...__fromsearch__1

Marcia



WOW- thanks for the link! It was a good read. I am especially interested in trying my cake decorating tools now after reading that thread!

~ Namaste ~

 

Home studio potter 

 

Shanel Pottery 

www.shanelpottery.com

www.facebook.com/shanelspottery 

 

 

 

"To me the greatest thing is to live beauty in our daily life and to crowd every moment with things of beauty.  It is then, and then only that  the art of the people as a whole is endowed with it's richest significance.  For it's products are those made by great a many craftsmen for the mass of the people, and the moment this art declines the life of the nation  is removed far away from beauty.  So long as beauty abides in only in a few articles created by a few geniuses, the kingdom of beauty is nowhere near realization."                                                                                 - Bernard Leach 

#4 Nancy S.

Nancy S.

    My day job pays for my clay habit

  • Members
  • PipPipPip
  • 232 posts
  • LocationHarrisburg area, PA

Posted 07 January 2013 - 01:11 PM

I am especially interested in trying my cake decorating tools now after reading that thread!


*grins* It's great fun once you get the right consistency of clay/slip. I also recommend perusing YouTube for gumpaste (fondant) flower tutorials -- sooo many techniques that should be adaptable to clay!

#5 bciskepottery

bciskepottery

    Advanced Member

  • Moderators
  • 2,663 posts
  • LocationNorthern Virginia

Posted 07 January 2013 - 07:10 PM


I am especially interested in trying my cake decorating tools now after reading that thread!


*grins* It's great fun once you get the right consistency of clay/slip. I also recommend perusing YouTube for gumpaste (fondant) flower tutorials -- sooo many techniques that should be adaptable to clay!



http://finemessblog....-with-slip.html

http://finemessblog....i-tried-it.html

#6 Benzine

Benzine

    Socratic Potter

  • Members
  • PipPipPip
  • 2,398 posts
  • LocationThe Hawkeye State

Posted 07 January 2013 - 09:54 PM


I am especially interested in trying my cake decorating tools now after reading that thread!


*grins* It's great fun once you get the right consistency of clay/slip. I also recommend perusing YouTube for gumpaste (fondant) flower tutorials -- sooo many techniques that should be adaptable to clay!


No need to adapt the techniques. Fondant is basically clay......at least it basically tastes like it....
"Anything worth believing, is worth questioning"

#7 Rebekah Krieger

Rebekah Krieger

    The extraordinary clay bender

  • Members
  • PipPipPip
  • 786 posts
  • LocationWisconsin

Posted 07 January 2013 - 10:33 PM



I am especially interested in trying my cake decorating tools now after reading that thread!


*grins* It's great fun once you get the right consistency of clay/slip. I also recommend perusing YouTube for gumpaste (fondant) flower tutorials -- sooo many techniques that should be adaptable to clay!


No need to adapt the techniques. Fondant is basically clay......at least it basically tastes like it....

LOL!! Try marshmallow fondant! It's not like the other plastic stuff! LOL
Also- I noticed that the clay dries pretty fast when trying to manipulate small pieces. Fondant retains it's moisture/ placidity. I have taken many cake flower classes and have som fondant stamps too! This could get fun! (now if only I could figure out how to make a lotus which was never taught in wilton courses! :-)

~ Namaste ~

 

Home studio potter 

 

Shanel Pottery 

www.shanelpottery.com

www.facebook.com/shanelspottery 

 

 

 

"To me the greatest thing is to live beauty in our daily life and to crowd every moment with things of beauty.  It is then, and then only that  the art of the people as a whole is endowed with it's richest significance.  For it's products are those made by great a many craftsmen for the mass of the people, and the moment this art declines the life of the nation  is removed far away from beauty.  So long as beauty abides in only in a few articles created by a few geniuses, the kingdom of beauty is nowhere near realization."                                                                                 - Bernard Leach 

#8 bciskepottery

bciskepottery

    Advanced Member

  • Moderators
  • 2,663 posts
  • LocationNorthern Virginia

Posted 07 January 2013 - 10:38 PM




I am especially interested in trying my cake decorating tools now after reading that thread!


*grins* It's great fun once you get the right consistency of clay/slip. I also recommend perusing YouTube for gumpaste (fondant) flower tutorials -- sooo many techniques that should be adaptable to clay!


No need to adapt the techniques. Fondant is basically clay......at least it basically tastes like it....

LOL!! Try marshmallow fondant! It's not like the other plastic stuff! LOL
Also- I noticed that the clay dries pretty fast when trying to manipulate small pieces. Fondant retains it's moisture/ placidity. I have taken many cake flower classes and have som fondant stamps too! This could get fun! (now if only I could figure out how to make a lotus which was never taught in wilton courses! :-)





#9 Rebekah Krieger

Rebekah Krieger

    The extraordinary clay bender

  • Members
  • PipPipPip
  • 786 posts
  • LocationWisconsin

Posted 07 January 2013 - 10:59 PM





I am especially interested in trying my cake decorating tools now after reading that thread!


*grins* It's great fun once you get the right consistency of clay/slip. I also recommend perusing YouTube for gumpaste (fondant) flower tutorials -- sooo many techniques that should be adaptable to clay!


No need to adapt the techniques. Fondant is basically clay......at least it basically tastes like it....

LOL!! Try marshmallow fondant! It's not like the other plastic stuff! LOL
Also- I noticed that the clay dries pretty fast when trying to manipulate small pieces. Fondant retains it's moisture/ placidity. I have taken many cake flower classes and have som fondant stamps too! This could get fun! (now if only I could figure out how to make a lotus which was never taught in wilton courses! :-)



http://www.youtube.c...h?v=HrzoE7NzPOE


My mouth was literall agape the entire time! What the hell did I just witness!?! Holy cow! And by the way you win the award for finding literally everything I needed! LOL

~ Namaste ~

 

Home studio potter 

 

Shanel Pottery 

www.shanelpottery.com

www.facebook.com/shanelspottery 

 

 

 

"To me the greatest thing is to live beauty in our daily life and to crowd every moment with things of beauty.  It is then, and then only that  the art of the people as a whole is endowed with it's richest significance.  For it's products are those made by great a many craftsmen for the mass of the people, and the moment this art declines the life of the nation  is removed far away from beauty.  So long as beauty abides in only in a few articles created by a few geniuses, the kingdom of beauty is nowhere near realization."                                                                                 - Bernard Leach 

#10 Nancy S.

Nancy S.

    My day job pays for my clay habit

  • Members
  • PipPipPip
  • 232 posts
  • LocationHarrisburg area, PA

Posted 08 January 2013 - 10:50 AM

http://finemessblog....-with-slip.html

http://finemessblog....i-tried-it.html


That's so freakin' cool!! So many ideas, so little time.... Posted Image




0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users