Posted 27 December 2012 - 09:43 AM

Sweet wife bought me a New Peter Pugger for Christmas. I have buckets of clay from projects gone bad. Clay is mixture of stoneware, earthernware, skosh of porcelan. As clay is all mixed together II would like to pug for a Raku mix. Will this be Ok for a Raku clay? Any comments from experienced potters would be appreciated.

#2 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,117 posts
  • LocationRed Lodge, Montana

Posted 27 December 2012 - 10:15 AM

If you can pug some grog into the mix it may improve the refractory requirements needed for a raku clay body. he earthenware and porcelain might be a bit dense compared to the stoneware. stoneware that I have used in the past has been good for raku but it had a good bit of various size mesh of grog.
Many types of earthenware do not contain much grog. Terra cotta usually does. Sometimes porcelain can survive raku but usually it can crack or daunt in the process.
nice Christmas present!


Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#3 Harry Potter

Harry Potter

    Member

  • Members
  • PipPip
  • 20 posts
  • LocationLouisiana and Mississippi

Posted 27 December 2012 - 12:17 PM

If you can pug some grog into the mix it may improve the refractory requirements needed for a raku clay body. he earthenware and porcelain might be a bit dense compared to the stoneware. stoneware that I have used in the past has been good for raku but it had a good bit of various size mesh of grog.
Many types of earthenware do not contain much grog. Terra cotta usually does. Sometimes porcelain can survive raku but usually it can crack or daunt in the process.
nice Christmas present!


Marcia



Thanks for your reply. Makes sense, a little extra grog wouldn't hurt regardless. Porcelain amount is very minimal.

#4 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,117 posts
  • LocationRed Lodge, Montana

Posted 27 December 2012 - 10:01 PM

Since you don't have much porcelain to add to this mix, why don 't you keep it if for a white slip base for you other work?

Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#5 Iforgot

Iforgot

    Advanced Member

  • Members
  • PipPipPip
  • 155 posts
  • LocationColorado

Posted 28 December 2012 - 02:30 PM

Uuummmm, I'd pug in some grog and sand of various mesh sizes and some kayanite. Oh, and some mica325.



Darrel
Derek VonDrehle

Raku, Pit fired, Majolica, and Stoneware ceramic artisit

#6 Harry Potter

Harry Potter

    Member

  • Members
  • PipPip
  • 20 posts
  • LocationLouisiana and Mississippi

Posted 28 December 2012 - 10:45 PM

Uuummmm, I'd pug in some grog and sand of various mesh sizes and some kayanite. Oh, and some mica325.



Darrel



Thanks for taking time to respond. I appreciate your input. Harry