Thanks Chris, for the suggestions.

I do have the manual for the kliln, I had not used the cone fire function because it does not have a hold at peak temp, I had been told by Skutt that I needed to hold for 10-15 min at 2200 for more even firing.

I have also talked to a man at a large S East show with beautiful cone6 elec glazes that said, "Lady,just hit ^6 and START and go back to the house".

 

 

My KilnMaster II on my new (this summer) Skutt 1018 allows holds in the cone fire mode. Check the manual again. In the Cone fire mode, after entering the preheat, the cone number, then the speed, there should be a hold prompt.

 

Good luck.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.