Pottery Walker Posted December 23, 2012 Report Share Posted December 23, 2012 Hello my fellow forum members, I was hoping for a little guidance as to what is a good cone 5/6 clay for large open body pieces, "large bowls ect' I have been using Laguna Clay "Calico" which I have found to be very inconsistent from bag to bag, and very weak. I would prefer to use an Aardvark Clay as they are the closest to me. I look forward to your responses. Thank You Link to comment Share on other sites More sharing options...
OffCenter Posted December 23, 2012 Report Share Posted December 23, 2012 For an all-purpose cone 6 white stoneware the best I've found after testing lots of commercial and from scratch bodies is Laguna's B-Mix. Jim Link to comment Share on other sites More sharing options...
Pottery Walker Posted December 24, 2012 Author Report Share Posted December 24, 2012 Jim, Thank You for the recommendation. I will probably give that a try. For an all-purpose cone 6 white stoneware the best I've found after testing lots of commercial and from scratch bodies is Laguna's B-Mix. Jim Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.