Interesting -- don't give up "grandma's" pyrex. Lessons on changes in basic materials and following directions regarding use apply to clay, also.

http://todayhealth.t...n-the-rise?lite

#2 Diana Ferreira

Diana Ferreira

    opinionated ignoramus

  • Members
  • PipPipPip
  • 186 posts
  • LocationCape Town, South Africa

Posted 21 December 2012 - 10:37 AM

yea, old Pyrex used to be made of Borosilicate glass. Sadly not today.
Diana
www.dianaferreiraceramics.com
https://www.facebook...70824173&type=3

#3 Diane Puckett

Diane Puckett

    Advanced Member

  • Members
  • PipPipPip
  • 398 posts
  • LocationAsheville, NC

Posted 21 December 2012 - 04:37 PM

Interesting article. Now I know it is not me just imagining the difference in newer Pyrex. In addition, the numbers came off my new Pyrex measuring cup I when I ran it through the dishwasher, and another Pyrex measuring cup dribbles when it pours. That was aggravating, but now I am afraid to even use them in the microwave.
Diane Puckett
Dry Ridge Pottery

#4 Mark McCombs

Mark McCombs

    Advanced Member

  • Members
  • PipPipPip
  • 123 posts
  • LocationSW Washington

Posted 21 December 2012 - 10:14 PM

I found this out the hard way several years ago.