I am loking a a blue glaze that would give several tinge of colors in firing. Do you have a nice recipe to share? My mother tongue is french so I am sorry if there are mistakes in my message!

 

Thank you very much!

Louise

 

 

Share this post


Link to post
Share on other sites

My favorite blue for red/dark brown clay bodies is Bright Sky Blue (Cone 6 Oxidation). On those clay bodies, the colors run from shades of blue to white. The recipe was developed by Ron Roy and John Hesselberth and can be found in their book, Mastering Cone 6 Glazes.

 

Miri , a potter in Puerto Rico, has done several glaze tests of variations of the Mastering Cone 6 Glazes and she has published their recipes on her blog site http://nickandmiri.wordpress.com/

 

You can also Google "Clayart archives" and search for blue glazes. Lots of recipes there.

Share this post


Link to post
Share on other sites

Check out:

 

http://rutileblue.blogspot.com/

 

web site in English and French

 

- h a n s e n -

 

 

Dear friends

 

I am loking a a blue glaze that would give several tinge of colors in firing. Do you have a nice recipe to share? My mother tongue is french so I am sorry if there are mistakes in my message!

 

Thank you very much!

Louise

 

 

 

 

 

 

Share this post


Link to post
Share on other sites

Louise,

Sorry I missed the ^6 reference. I got mixed up with Eric's link to Eduoard's blog which is for ^9 Reduction glazes, I believe.

 

Here is a nice satin matt base glaze for ^6. The added colorants are for ^6 Reduction.

For a stronger blue , increase the cobalt. There will be lavender tinges because of the Magnesium in the Dolomite.

You could try using a blue mason stain and see what happens.

 

Selsor’s ^6 R Semi Matt

 

EPK 20.3

 

Dolomite 17.7

 

Neph. Syen. 33.6

 

Silica 15.9

 

Whiting 3.5

 

Ger, Borate 8.8

 

99.8

 

Takes colors well

 

Blue/lavender

 

1% cobalt Carb

 

Lt green 1.5% Nickel Carb

 

1.5% Rutile

 

Lt. Blue gray

 

0 .5% cobalt carb.

 

2.5% rutile

 

gray 2.5 rutile

 

2.5 nickel carb.

Share this post


Link to post
Share on other sites

Look in : http://ceramicartsdaily.org/category/ceramic-glaze-recipes/mid-range-glaze-recipes/

 

hansen

 

Hello Louise,

 

If your are oxidation cone 6 firing you can use the floating blue of James Chappell - http://floatingblue.blogspot.com/

 

It is very reliable, very interesting glaze. Right now I am in a hurry, but you may also contact me on judith.st@gmail.com for the receipe in french if you like.

A plus, Judith

 

 

 

 

Share this post


Link to post
Share on other sites

Thanks for the shout-out Bruce! I just mixed up 5 more tests based on Mastering cone 6 Glazes (4 blues and 1 green). Have to fire a bisque first before I get to test them out but I'll be sure to post photos here of my results. I'm liking this forum! :-)

 

Miri

 

 

My favorite blue for red/dark brown clay bodies is Bright Sky Blue (Cone 6 Oxidation). On those clay bodies, the colors run from shades of blue to white. The recipe was developed by Ron Roy and John Hesselberth and can be found in their book, Mastering Cone 6 Glazes.

 

Miri , a potter in Puerto Rico, has done several glaze tests of variations of the Mastering Cone 6 Glazes and she has published their recipes on her blog site http://nickandmiri.wordpress.com/

 

You can also Google "Clayart archives" and search for blue glazes. Lots of recipes there.

 

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.