Hello

I had made a big tile and it's plaster mold, I didn't take it off and the clay is almost dry
and do not know how to remove it, I wish not to hurt the plaster in the process, do you some suggestions?

THANKS!

#2 minspargal

minspargal

    Advanced Member

  • Members
  • PipPipPip
  • 90 posts
  • LocationPort Aransas, Tx

Posted 12 December 2012 - 04:09 PM

Try spraying the clay with water to soften it up again, pull it off and start over.

#3 perkolator

perkolator

    Advanced Member

  • Members
  • PipPipPip
  • 355 posts
  • LocationCalifornia

Posted 12 December 2012 - 04:15 PM

yeah, you can soften the clay up a bit and try to remove - but you'll have to dry it out longer to cure the mold before using. i recommend trying to use an air hose if you have access to air compressor - stream your air between the clay and plaster to try to release w/o damaging the plaster with tools. you can also use a damp sponge to remove clay from your plaster.

#4 claclana

claclana

    Advanced Member

  • Members
  • PipPipPip
  • 60 posts
  • LocationBuffalo, NY

Posted 12 December 2012 - 06:55 PM

alright, I will try it!
thank you! Posted Image




0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users