Bisque Misfire?

Recommended Posts

paige    0

Yesterday I fired my Paragon snf243 - attempting cone 05, no watcher - and I set the knobs incorrectly. They should have been 5 - 1- 2, for 5 -6 hours, but I did 1 - 1- 2 for 7 hours. I don't know why my brain wasn't working, but that's another problem entirely. The kiln sitter never tripped and the little cone doesn't appear to have bent.

 

Should I refire or assume that it still got pretty hot enough? What does that first (top) knob determine?

 

Thanks for the help!

Share this post


Link to post
Share on other sites
Marcia Selsor    1,301

I am not familiar with what 5-1-2 or 1-1-5 is.

But if you didn't hit temperature, just refire using the right settings. If it doesn't work a second time, maybe you need new elements.

 

Marcia

Share this post


Link to post
Share on other sites
paige    0

Well that first knob is the power level, so at min setting, I doubt it got very hot. I just restarted it. Oi.

 

I am not familiar with what 5-1-2 or 1-1-5 is.

But if you didn't hit temperature, just refire using the right settings. If it doesn't work a second time, maybe you need new elements.

 

Marcia

 

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×