What do i need to add to my cone 6 stoneware clay to make it suitable for slipcasting? I have a trash can full of waste clay that is not worth my time to wedge.

 

 

 

I usually buy slip when I need it. I never make it. However you can 'Google' 'Paul Wandless slip making'. He has a method of making your moist clay into casting slip. You may get the same info here on CAD; try a search.

Share this post


Link to post
Share on other sites

I'd like to learn more about slipcasting, but am having trouble finding information on it.

 

 

 

Try doing a library or Google search on 'mold making for ceramics' and there you will find slipcasting information.

Share this post


Link to post
Share on other sites

Richard Notkin is having summer workshops in Helena. He is one of the best mold makers in the business.

Work with a Master: Plaster Moldmaking / Ceramic Casting One two-week session only: June 10-21, 2013 (Limited to nine participants)

- Plaster technology & optimum mixing techniques - Prototype design & mold fabrication - Complex multiple piece mold mechanics - Press molding & slip-casting - Keys, pouring/draining systems, vents, etc. - Slip formulation & deflocculation- Altering/combining/assembling unique castings - Industrial/mass production techniques - Unusual/experimental techniques, and much more...

Tuition: $850. For more information contact: notkin@dishmail.net Studio/materials fee: 125. Or send SASE to: Richard Notkin TOTAL: $975. P.O. Box 698( Motel available, two weeks: $350./double, $700./single, or limited rooms in local homes, prices vary) Helena, MT 59624-0698

 

 

Marcia

I'll post this under events, too

Share this post


Link to post
Share on other sites

You can make most clays into a slip body but it will not be the best slip body-I suggest if you want trouble free slip results us a slip body made for slipping. Waste clay is not great slip clay-You can use it but it will take some time and test results it may work out and it may not. I have either made slip clay from scratch dry materials or bought slip clay in dry state but never tried to make whatever I was throwing into a slip body.

Mark

Share this post


Link to post
Share on other sites

John B. Kenny's Complete Book of Pottery Making has directions for making casting slip that involves a 10 day process. This is an old book from the 1950s.

It begins with a dry powder clay recipe plus diffloculent additives and proper blending of 10 minutes three times /day for 10 days. I used this process and it was very successful . I was able to make slip for particular clay bodies.

 

Marcia

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.