Posted 06 December 2012 - 11:15 AM

Has anyone tried using Rub and Buff on their ceramics?

#2 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,088 posts
  • LocationRaleigh, NC

Posted 06 December 2012 - 11:22 AM

Yes, I have used it on non functional pieces to add color and it works well. I rakued some elephants that came out too evenly dark grey so I used the silver to add highlights. It was a bit unforgiving on the non glazed surface ( sank in and stayed put ) but I imagine you could control it better on a glazed surface. I've also used the copper color with good results.
Chris Campbell Pottery
Contemporary Fine Colored Porcelain
http://ccpottery.com/

>TRY ... FAIL ... LEARN ... REPEAT"

" If a sufficient number of people are different, no one has to be normal "

Fredrick Bachman

#3 Lucille Oka

Lucille Oka

    Advanced Member

  • Members
  • PipPipPip
  • 756 posts
  • LocationCalifornia

Posted 06 December 2012 - 11:17 PM

Yes. I have used Rub and Buff on a lamp base, clay and wood sculptures, plaster casts, and other 'objets d'art'. I have also used it to alter colors.
R 'n' B can be thinned (read the package). It goes on smoothly with good coverage and makes a nice sheen when buffed. However it is not to be used on products made for food service.