I looked at my glazed pieces in the kiln when it was at 400 degrees, and 2 of the pieces had water crystals growing out of the top. I turned the kiln off for an hour, took a nap, and they were still there. The kiln is at 600 degrees and they are still there. Is this normal? Maybe I usually just dont check on my work when its in the kiln.

Share this post


Link to post
Share on other sites

Justin there are no 'water crystals' (ice) that can survive at 400, 600, or 800 degrees. Water evaporates at 212 degrees F. and turns to steam.

 

What glaze is this? It looks to me like debris from the bottom of a glaze vat, or some of the crystals that can be found in glazes that have them in the mix. They also look deliberately placed and spaced.

The bits are quite large it's a wonder that you didn't see them when you applied the glaze.

Share this post


Link to post
Share on other sites

Lucille, it none of those.....As I said they just grew. They are a little bigger than course sea salt. This is a shino over a blue, and when i do this combination, the glaze tends to have pin holes in it before the fire (due to air bubbles), but they go away. Im wondering if the blue from the first dip is pushing some sort of molecule through the little holes. The kiln is at about 1200 degrees now, so i will see if anything weird happened soon when i open the kiln on thursday.

Share this post


Link to post
Share on other sites
Guest JBaymore

Is this a commercial glaze "shino"?

 

Looks like borax chunks or soda ash chunks (usually it fully dissolves in the glaze water and is evenly distributed).

 

Was the glaze seived through at least 80m before use? Had the glaze sat around a long time and had "dry stuff" possibly on the sides of the container?

 

best,

 

...............john

Share this post


Link to post
Share on other sites

went through a 60 mesh sieve........i shook it well, and only dipped down a little........1.5 month old glaze. may have made diamonds, jk. It's only 9 am here, and been up all night......time to throw more!

Share this post


Link to post
Share on other sites

Not sure why one would look or care at 400 degrees but how did it look after going to cone 6? Was it normal looking then?

Looks like crystals but they are not from water at that temp. They most likely laid down at cone 6?

How is the piece after a normal fire?

Mark

Share this post


Link to post
Share on other sites
Guest JBaymore

They disappeared after a cone 6 fire.....I guess it is normal for my glaze.

 

 

On close examination there is absolutely no trace of a surface mottling or texture difference or anything like that which would indicate the location of those concentrations of a particular material?

 

best,

 

......................john

Share this post


Link to post
Share on other sites

I think John is on to something with the soda ash material. I just mixed up a Cone 10 Shino glaze with soda ash in it. I put one third water in the bottom of the bucket and then dumped in all my materials for the glaze. I went to stir with my propeller. The glaze was crashing around the sides. I looked in. The soda ash had formed huge rocks like salt crystals. I removed the large chunks, reseived the glaze, but did not feel confident about using it with so much of one material removed. I had to remix the entire 10,000 gram batch. I tested both glazes .They look pretty much the same!

I guess the advice for you would be to smooth the surface with your thumb before you fire, and DON'T LOOK INTO THE KILN!

TJR

Share this post


Link to post
Share on other sites
Guest JBaymore

Soda ash is 100% soluble in water. But if it is the granular form, sometimes it is used before it dosolves. And sometimes the soda ash crystallizes out on the edges of the dry glaze on the container edges. Then it can fall back into the glaze on application... and cause concentrations of soda ash in localized areas.

 

But I would expect tehre tto be some trace of this concentration of the flux on the surface of the fired glaze.

 

best,

 

 

...................john

 

 

 

PS: BTW.... when I mix my main shino, all of the soda ash is first fully dissolved in hot water before adding that water into the overall wet glaze batch and stirred in. If you do this... be CAREFUL ... that concentrated soda ash/water solution is NOT good to get on your skin and particularly not good to splash in you eyes.

Share this post


Link to post
Share on other sites

Soda ash is 100% soluble in water. But if it is the granular form, sometimes it is used before it dosolves. And sometimes the soda ash crystallizes out on the edges of the dry glaze on the container edges. Then it can fall back into the glaze on application... and cause concentrations of soda ash in localized areas.

 

But I would expect tehre tto be some trace of this concentration of the flux on the surface of the fired glaze.

 

best,

 

 

...................john

 

 

 

PS: BTW.... when I mix my main shino, all of the soda ash is first fully dissolved in hot water before adding that water into the overall wet glaze batch and stirred in. If you do this... be CAREFUL ... that concentrated soda ash/water solution is NOT good to get on your skin and particularly not good to splash in you eyes.

 

John;

Thanks for the tip re hot water and soda ash. I did want to take a picture of the big rocks that it formed. Might be an old material. I always premix my bentonite before adding to the already wet glaze materials. I will remember to use hot water the next time I mix the Shino, and pre-mix the soda ash.

Tom[TJR]

Share this post


Link to post
Share on other sites

ok.....so my brother used it a week ago, and it came out fine after the fire, but we could see crystals all over it before putting it in the fire, and he said it was hard to work with. So i decided to mix it up really good, then run it through a 60 mesh sieve. the problem is that only about 80% of the glaze is going through, and it is leaving behind a gritting mess that i have to scrape off. I'm really concerned that this is going to mess up the COE. Would it be better to not put it through the sieve and use it as is? Any other ideas? Help please!!!

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.