I would like to make a lava glaze that fires to cone 9. I would appreciate some advice. Can I use any glaze and add some silica carbide ( how much)? I have seen amy lava glazes for up to cone 6, but not above that.

 

Thanks in advance.

 

Lynette

Share this post


Link to post
Share on other sites

i'm going to go out on a limb here and say that's a definite maybe.

 

iirc i tried amounts less than 1% with a volcanic ash base at ^8-9 in oxidation. the result was more sponge toffee than lava.

 

apparently particle size can seriously affect the outcome

 

*from what i read fine particle size can encourage localised reduction but i put silicon carbide down at sponge toffee.

 

 

 

 

I realized after I asked this question, that, it will not work with any glaze, because I have used it tocause localise reduction and that glaze did not crater. Ther must be a certain chemistry that is necessary, but I havn't been able to find much information about high fire crater glazes.

 

Lynette

Share this post


Link to post
Share on other sites

My teacher obtained it from an industrial type place... something to do with glass.

 

I'm doing some tests now. We're doing them as an addition to the slip – not the glaze. He recommended an addition of around 6%. In the tests, they range from 2% to 12%. I also did mixes with other glazes, to see what happens.

 

 

edit: I found a link to a rock tumbler website, http://rocktumbler.com/grit.shtml They have the type that we used, the coarsest grit.

Share this post


Link to post
Share on other sites

Ok, so I did a few test glazes @ cone 10 with a cratering slip. It didn't do anything, as a slip or a glaze... in any of the tests. This particular example was dipped in slip that had the SC, bisqued, and then glazed.

 

I have a feeling that we had the wrong material, though. I'll find out the next time I'm at school.

 

8274108860_b3fb2e96df_n.jpg

Ceramics by avaviel, on Flickr

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.