timbo_heff    37

Anyone have a Shino formula that is known to work well on bone dry wares?

I am hoping to avoid bisque firing but I guess I will if I have to .

I have some of this Gustin shino made up ... (not sure if Chris actually had anything to do with it )

:

Could this maybe be tweaked to work on bone dry with the addition of bentonite ?

Gustin Shino

Nepheline syenite-45%

F-4 Soda feldspar-10.8%

Spodumene-15.2%

OM # 4 ball clay-15.0%

EPK-10.0

Soda ash-4.0%

 

Perhaps bisque fire is the best option no matter what if the wares are already bone dry ?

 

Thanks in advance for any advice on this !

Share this post


Link to post
Share on other sites
JBaymore    1,432

Tim,

 

Maybe if you used calcined kaolin for all of the ball clay. Still iffy though. Test.

 

best,

 

......................john

Share this post


Link to post
Share on other sites
timbo_heff    37

Tim,

 

Maybe if you used calcined kaolin for all of the ball clay. Still iffy though. Test.

 

best,

 

......................john

 

 

Thanks John ! ... as I suspected / feared ... bisque it will be

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×