Anyone have a Shino formula that is known to work well on bone dry wares?
I am hoping to avoid bisque firing but I guess I will if I have to .
I have some of this Gustin shino made up ... (not sure if Chris actually had anything to do with it )
:
Could this maybe be tweaked to work on bone dry with the addition of bentonite ?
Gustin Shino
Nepheline syenite-45%
F-4 Soda feldspar-10.8%
Spodumene-15.2%
OM # 4 ball clay-15.0%
EPK-10.0
Soda ash-4.0%

Perhaps bisque fire is the best option no matter what if the wares are already bone dry ?

Thanks in advance for any advice on this !

#2 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,172 posts
  • LocationWilton, NH USA

Posted 04 December 2012 - 05:09 PM

Tim,

Maybe if you used calcined kaolin for all of the ball clay. Still iffy though. Test.

best,

......................john

John Baymore
Adjunct Professor of Ceramics; New Hampshire Insitute of Art

Former Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#3 timbo_heff

timbo_heff

    Advanced Member

  • Members
  • PipPipPip
  • 205 posts
  • LocationMA / NY

Posted 06 December 2012 - 09:17 AM

Tim,

Maybe if you used calcined kaolin for all of the ball clay. Still iffy though. Test.

best,

......................john


Thanks John ! ... as I suspected / feared ... bisque it will be