What happens to wax resist in a kiln?


  • Please log in to reply
2 replies to this topic

#1 justin1287

justin1287

    Advanced Member

  • Members
  • PipPipPip
  • 63 posts
  • LocationColorado

Posted 28 November 2012 - 01:40 PM

does it completely evaporate, or does it leave residue left behind?

#2 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,359 posts
  • LocationRed Lodge, Montana

Posted 28 November 2012 - 02:26 PM

Yes, it should completely burn off.

Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#3 TJR

TJR

    Advanced Member

  • Members
  • PipPipPip
  • 1,821 posts
  • LocationWinnipeg,Manitoba,Canada

Posted 28 November 2012 - 07:10 PM

Should burn off. Make sure your kiln is vented.
Tom.[TJR]