Posted 15 November 2012 - 10:41 PM

In general is it unsafe to use unglazed stoneware for food?

#2 OffCenter

OffCenter

    Advanced Member

  • Members
  • PipPipPip
  • 1,372 posts

Posted 15 November 2012 - 10:47 PM

In general is it unsafe to use unglazed stoneware for food?


No.

Jim
E pur si muove.

"But it does move," said Galileo under his breath.

#3 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,125 posts
  • LocationWilton, NH USA

Posted 16 November 2012 - 10:32 AM

What he said.

best,

....................john

John Baymore
Professor of Ceramics; New Hampshire Insitute of Art

Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#4 bciskepottery

bciskepottery

    Advanced Member

  • Moderators
  • 2,671 posts
  • LocationNorthern Virginia

Posted 16 November 2012 - 11:02 AM

Little confused by the syntax . . . unsafe to use unglazed or safe to use unglazed? What kind of food -- dry (breads, etc) or liquid (soups, sauces, etc)?

There have been a few posts lately about using unglazed for food . . . the thought of a knife or spoon scraping across an unglazed surface is giving me flashbacks school days and fingernails skreeching across the blackboard.

#5 Nancy S.

Nancy S.

    My day job pays for my clay habit

  • Members
  • PipPipPip
  • 232 posts
  • LocationHarrisburg area, PA

Posted 16 November 2012 - 02:56 PM

Little confused by the syntax . . . unsafe to use unglazed or safe to use unglazed? What kind of food -- dry (breads, etc) or liquid (soups, sauces, etc)?

There have been a few posts lately about using unglazed for food . . . the thought of a knife or spoon scraping across an unglazed surface is giving me flashbacks school days and fingernails skreeching across the blackboard.


*laughs* Oh, man! You just made my skin crawl... O_o

I use unglazed ^6 clay, fired to ^6, for salt piggies. Seems to work pretty well. I also use the same clay only fired to ^06 (more absorbent that way) for sugar keepers - also works well. So while they're not in contact with liquids, they're also not being used with utensils.

#6 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,125 posts
  • LocationWilton, NH USA

Posted 16 November 2012 - 03:12 PM

Not everyone uses metal eating implements, nor does everyone use forks, spoons, and knives.

best,

...................john

John Baymore
Professor of Ceramics; New Hampshire Insitute of Art

Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#7 koreyej

koreyej

    Advanced Member

  • Members
  • PipPipPip
  • 49 posts
  • LocationBouton, Iowa

Posted 20 November 2012 - 12:16 PM

Funny question. Isn't that what Pampered Chef's ware is? Personally, I like my ware glazed. However, they offer a lot of ovenware that is not glazed and sell it as food safe. Maybe worthy of some investigation?