Jump to content


Photo
- - - - -

Switching between 2 K type pyrometer probes with one meter.


  • Please log in to reply
9 replies to this topic

#1 docweathers

docweathers

    Gismo Guy

  • Members
  • PipPipPip
  • 643 posts
  • LocationSpokane Wa

Posted 14 November 2012 - 12:44 PM

I have a pyrometer that accommodates 1 type k probe. I would like to add a second probe by having a switch to go from one to the other.

Is it sufficient to have a single pole double throw switch to change the connection for one of the probe leads (while the other one remains continuously connected) or do I need to use a double pole double throw switch to change the connection for both leads simultaneously.

I asked the vendor and I got basically a "darned if I know"

Thanks Larry

Larry

Lawrence Weathers

Gismo Guy

Spokane WA


#2 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 5,050 posts
  • LocationGrayslake, IL

Posted 14 November 2012 - 01:32 PM

Both the positive and negative leads will have to be switched. There is no common.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]


#3 docweathers

docweathers

    Gismo Guy

  • Members
  • PipPipPip
  • 643 posts
  • LocationSpokane Wa

Posted 14 November 2012 - 03:23 PM

Will do

Thanks

Larry

Lawrence Weathers

Gismo Guy

Spokane WA


#4 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,266 posts
  • LocationWilton, NH USA

Posted 15 November 2012 - 10:30 AM

If accuracy matters to you, it also needs to be a switch made for actual thermocouple switching. So for Type K use, the metals in the switch need to be Chromel / Alumel compatible. (and get the right wire to the right metal ;)src="http://ceramicartsda...ault/wink.gif"> on the switch) Copper components don't "cut it".

Otherwise you create secondary thermocouples (two joined dis-similar metals) at the junctions between the thermocouple extension wire (which ALSO needs to be the correct stuff) and the switch. As the temperature in the area of the SWITCH changes,.... you create another set of electromotive forces...... and this impacts the reading that you will get on the meter.

Gold and silver contacts on the good qulaity types of switches minimize this issue.....but make them pricey.

http://www.omega.com...SW14&Nav=temg16


Another potential solution is to use a simple patch panel. Not quite as elegant, but also works

http://www.omega.com...DRTB&Nav=temg16

best,

................john

John Baymore
Adjunct Professor of Ceramics; New Hampshire Insitute of Art

Former Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#5 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,311 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 15 November 2012 - 01:02 PM

It would be easy to just pick up a used fluke on e bay that has two meter leads-they run about 50-65$
Get the older box style I have three and they work great.
Mark
Mark Cortright
www.liscomhillpottery.com

#6 docweathers

docweathers

    Gismo Guy

  • Members
  • PipPipPip
  • 643 posts
  • LocationSpokane Wa

Posted 15 November 2012 - 03:45 PM

It would be easy to just pick up a used fluke on e bay that has two meter leads-they run about 50-65$
Get the older box style I have three and they work great.
Mark



That's a good idea. I'm not familiar with fluke pyrometer's. What model numbers are the old style box that you recommend?

Larry

Lawrence Weathers

Gismo Guy

Spokane WA


#7 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,311 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 15 November 2012 - 05:26 PM

Model
Fluke 52-it takes two probes-from two source points.
I also use the fluke 51-takes single probe

You will need two yellow plugs that take the wire and plug into this meter. You can also get them from fluke

These meters are cheap used on E-Bay-
They are an older model but are well made and function well.
Mark
Mark Cortright
www.liscomhillpottery.com

#8 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,311 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 15 November 2012 - 07:47 PM

Doc W
when you are ready to get new burners heres a place I have been dealing direct with for 30 plus years on small cheaper venturi burners.
Gas appliance Co
phone# 951 940- 5252


They sell small MR 75,000 and MR 100,000 btu burners
They are on several kilns I operate.
Mark
Mark Cortright
www.liscomhillpottery.com

#9 docweathers

docweathers

    Gismo Guy

  • Members
  • PipPipPip
  • 643 posts
  • LocationSpokane Wa

Posted 15 November 2012 - 10:10 PM

Doc W
when you are ready to get new burners heres a place I have been dealing direct with for 30 plus years on small cheaper venturi burners.
Gas appliance Co
phone# 951 940- 5252


They sell small MR 75,000 and MR 100,000 btu burners
They are on several kilns I operate.
Mark


It's my understanding that I would have to do a major overhaul of the manifold to accommodate these burners. Is that true?

Larry

Lawrence Weathers

Gismo Guy

Spokane WA


#10 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,311 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 16 November 2012 - 01:16 AM


Doc W
when you are ready to get new burners heres a place I have been dealing direct with for 30 plus years on small cheaper venturi burners.
Gas appliance Co
phone# 951 940- 5252


They sell small MR 75,000 and MR 100,000 btu burners
They are on several kilns I operate.
Mark


It's my understanding that I would have to do a major overhaul of the manifold to accommodate these burners. Is that true?


That may be true-I do not know what it looks like exactly-the small burners are about 7 1/2 -8 inches long-
New manifold is not that much to re-plumb if it fixes the kiln.
I run 8 of the small ones on a 35 cubic foot car kiln so 4 would be plenty -if not overkill.
Mark
Mark Cortright
www.liscomhillpottery.com