from this past weekend, we loaded the anagama at Blue Mountain, outside Missoula, MT

 

the kiln is owned by the Clay Studio of Missoula

 

at least 1000 pieces got in there, it is quite big, i will get some better pics of the whole kiln when i take my shift next friday

 

305616_175009162638922_1131185662_n.jpg

 

423115_174832479323257_403821196_n.jpg

 

 

 

couple of my sculpture on the floor there, in between the stokes! ^^^^ should be interesting if they dont get creamed by people sidestoking....

 

 

 

262072_174832352656603_374060877_n.jpg

 

 

557595_174832605989911_1143184024_n.jpg

 

 

207503_174832759323229_1816291454_n.jpg

 

 

fires until next sunday afternoon, opening party the following sunday

Share this post


Link to post
Share on other sites

Nicely stacked! How long is your shift? I help fire Roger Jamison's anagama in Juliette, Georgia and usually take 3 six-hour shifts with another person. If this video still works it condenses a 6-day firing and unloading down to a few minutes: http://www.rogerjami...ndex.php/video/ The camera angle makes the kiln look shorter and fatter than it is. The unloading through the side door shows the size better.

 

Jim

Share this post


Link to post
Share on other sites

willdo! i am really excited about this fire...they did some modifications to the flue and firebox a few fires ago and i hear these last few fires have been superb, plenty hot and the kiln really hums

 

friday when i go back it should be the peak, i may just stay til the fireoff on sunday

 

so glad to be back in the Wood! its been 3 years since my last woodfire, i have 3 of 4 sculptures in there, and about 20 functional pieces for the household, tumblers and bowls for our everyday use

 

wooooop!

 

edit: crosstyping with you Offcenter....i have midnight to 6am friday, then also noon to 6 pm saturday! stoked!

Share this post


Link to post
Share on other sites

willdo! i am really excited about this fire...they did some modifications to the flue and firebox a few fires ago and i hear these last few fires have been superb, plenty hot and the kiln really hums

 

friday when i go back it should be the peak, i may just stay til the fireoff on sunday

 

so glad to be back in the Wood! its been 3 years since my last woodfire, i have 3 of 4 sculptures in there, and about 20 functional pieces for the household, tumblers and bowls for our everyday use

 

wooooop!

 

edit: crosstyping with you Offcenter....i have midnight to 6am friday, then also noon to 6 pm saturday! stoked!

 

 

Have fun. Hope it is a great firing. Post pics.

 

Jim

Share this post


Link to post
Share on other sites

in full fire....

 

Capture-8.jpg

 

Perry Haas is the current woodfire resident at the Missoula Clay Studio, here is some of his work from previous fires

 

Capturekloii.jpg

 

___________________________________________________________

 

Capturehgfghdf.jpg

 

___________________________________________________________

 

Capturejghjfdgd.jpg

 

 

if we acheive any surfaces like that this time, its all good!

Share this post


Link to post
Share on other sites

it is about a 2.5 hour drive for me, well worth it

 

claystudio of missoula is a great place, spent the evening before the loading there, glazing my stuff and hanging out, very good atmostphere, and the residents are doing some high quality work, especially perry

 

it is SO difficult to be up here while the fire is going, i want to be in front of that firebox chucking wood, right NOW, lol...c'mon friday!

Share this post


Link to post
Share on other sites

variable, but it think they will fire 3-4 more times before next august

 

483125_523721100971571_1622195347_n.jpg

 

 

its warming up in there, latest shot on the web, from a few minutes ago....that is the light of the porch fire, probably going to push it inside pretty soon

Share this post


Link to post
Share on other sites

yours truly sidestoking toward the end..

.305583_10151247121737445_500730259_n.jpg

 

we finished up 12 hours early...^12 bent in front...^11 down in the middle, ^11 bending in the back, that was the last time we looked a few hours before the mega fire-off

 

306040_176990929107412_1263485883_n.jpg

 

 

 

540122_10151246197272445_701923680_n.jpg

 

 

 

 

nice view too

 

188565_10151247111412445_2120109538_n.jpg

 

 

 

opening is in 2 weeks! dec 1....last time they tried to go in after only 1 week and everyone was melting their shoes-soles, lol

Share this post


Link to post
Share on other sites

haha, YES, Fyaaah!

 

that was the very last stoke, when we filled all the sidestokes, then chucked (gently) about 50 logs int the front firebox, then shut the flue...crazy reduction for a bit (and the flames coming out all over. then re-opened, re-closed flue...crazy-fun time

Share this post


Link to post
Share on other sites

here we are at the end, tag-teaming to get as much wood in as possible before our gloves lit on fire!

 

283324_10151247123172445_1652294466_n.jpg

 

 

perry's foam trucker hat and moccassins may not meet the highest safety standards

Share this post


Link to post
Share on other sites

here we are at the end, tag-teaming to get as much wood in as possible before our gloves lit on fire!

 

283324_10151247123172445_1652294466_n.jpg

 

 

perry's foam trucker hat and moccassins may nor meet the highest safety standards

 

too cool T

Share this post


Link to post
Share on other sites

"perry's foam trucker hat and moccassins may not meet the highest safety standards"

 

Really? That's somewhat of a concern, as my safety equipment is made from an old pair of moccasins lined with the foam from a trucker hat........ I may have to upgrade to using an old pair of Crocs lined with bits of a Snuggie.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.