Technically, some high-end digital scales can be more accurate than a triple-beam. However, I think that the difference is negligible for the amounts that go into most glaze recipes. Triple-beams are arguably more robust- this is a consideration if you're worried about spills.

 

If you're making test recipes in the 100 gram range- or smaller- a scale that goes below 1 gram might be (theoretically) useful- but I don't think that a 0.5 gram difference is going to wreck your recipe in too many cases...

Share this post


Link to post
Share on other sites

Digital will give you a greater range than triple beam, which is nice when measuring whole buckets of glaze. The only time less than 1 gram will be an issue is when measuring small test batches with small amount of colorants, like 0.25% cobalt carbonate. Ideally, you want something that can do as little as 1/10 gram and up to least 10 pounds. That will work for small test batches and full buckets.

Share this post


Link to post
Share on other sites

My Ohaus triple beam gets down to 1/10 of a gram-built like a tank

My Ohaus digital is the large capacity and does not spilt a gram much but does 5000 grams total.

Ohaus does make two smaller digital scales that I recall go smaller-I got mine from Baileys

Mark

Share this post


Link to post
Share on other sites

Technically, some high-end digital scales can be more accurate than a triple-beam. However, I think that the difference is negligible for the amounts that go into most glaze recipes. Triple-beams are arguably more robust- this is a consideration if you're worried about spills.

 

If you're making test recipes in the 100 gram range- or smaller- a scale that goes below 1 gram might be (theoretically) useful- but I don't think that a 0.5 gram difference is going to wreck your recipe in too many cases...

 

Thank you Most helpful!

Share this post


Link to post
Share on other sites

Technically, some high-end digital scales can be more accurate than a triple-beam. However, I think that the difference is negligible for the amounts that go into most glaze recipes. Triple-beams are arguably more robust- this is a consideration if you're worried about spills.

 

If you're making test recipes in the 100 gram range- or smaller- a scale that goes below 1 gram might be (theoretically) useful- but I don't think that a 0.5 gram difference is going to wreck your recipe in too many cases...

 

Thank you Most helpful!

 

 

No problem... but note Neil's comment (above) about cobalt carb and other high-impact colorants...

Share this post


Link to post
Share on other sites

I use an AND FW 100K for batches, it is accurate to 10g. For test batches I use an Ohaus dial-O-gram, it's accurate to 1/10th of a gram. For clay I use a cheap postal scale. At work we have a beam scale that is very nice, but I can't remember the make. It is quite old.

 

I like digital scales, but they are expensive. Outside of the postal scale I got my scales used and quite cheap. I really like the platform scale since it is digital, easy to tare, and has a large working area. The dial-O-gram is the way to go for a triple beam, IMO. It's fast and tares out easy for a beam scale.

 

Joel.

Share this post


Link to post
Share on other sites

I was told by multiple people that for glazes there is nothing better than a triple beam. If you purchased a super acurate digital with micro gram measures then I suppose, but my Ohaus is nicely built and is teh best in my mind.

 

I am a beginner so I am speaking from recommendations from those that have been doing this for many many years, and my few weeks of experience.

 

 

 

Good luck.

Share this post


Link to post
Share on other sites

My Ohaus gave out after 30 years, Ohaus told me the magnets were bad, so I decided to go digital. I would recommend buying one that is 150gX.01g for test glazes I have a American Velocity and the lid flips over and makes a tray for your chemicals. For mixing up batches of glaze I have a American Weigh 3000gX0.1g it has a bowl with it. I have been very pleased with both units, my tests and bigger batches are accurate.

Share this post


Link to post
Share on other sites

I have had my triple beam O'haus for over forty years. it has travelled from early stages of my pottery business in Upstate NY, to my personal studio in Montana and now in Texas. It does measure 0.1 gram and if you are doing smaller amounts for tests, you can take that 0.1 and divide it into smaller quantities visually.

I have additional weights that allow quantities up to 2110 grams to be measured at once. Digital scales may do that we'll also. Look on LabX.com for some scales and balances. I have seen all sizes of digital scales there and often triple beam balances. they are listed under lab equipment scales and balances.

As to your needs, you have to determine what quantities you plan to mix.

 

Marcia

Share this post


Link to post
Share on other sites

If you get a triple beam, make sure it has a tare poise. With it you can zero out the weight of the container you're using to weigh in. I use a little 3 inch wide dish that holds about 100 grams when doing small test batches. Very convenient.

Share this post


Link to post
Share on other sites

I had an aggravating day with a digital scale at work today so I thought it appropriate to note that when you buy a digital scale you might want to find one that doesn't click off when you are in between materials during a test, augggggg. I would put a chemical in the beaker then get another chemical and while my back was turned the evil thing would time out and turn off. Pure evil I tell you!

 

Joel.

Share this post


Link to post
Share on other sites

Alice,

 

I don't know that there is one. I'll look though. It is another guy's scale and I'm not that familiar with it. Now that you mention it I think I'll turn it over and see if there is a shut off for the time out feature. Thanks!

 

Joel.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.