      Ceramic Arts Network is looking for two new forum moderators for the Clay and Glaze Chemistry and Equipment Use and Repair sections of the Ceramic Arts Network Community Forum. We are looking for somebody who is an active participant (i.e. somebody who participates on a daily basis, or near daily) on the forum. Moderators must be willing to monitor the forum on a daily basis to remove spam, make sure members are adhering to the Forum Terms of Use, and make sure posts are in the appropriate categories. In addition to moderating their primary sections, Moderators must work as a team with other moderators to monitor the areas of the forum that do not have dedicated moderators (Educational Approaches and Resources, Aesthetic Approaches and Philosophy, etc.). Moderators must have a solid understanding of the area of the forum they are going to moderate (i.e. the Clay and Glaze Chemistry moderator must be somebody who mixes, tests, and has a decent understanding of materials). Moderators must be diplomatic communicators, be receptive to others’ ideas, and be able to see things from multiple perspectives. This is a volunteer position that comes with an honorary annual ICAN Gold membership. If you are interested, please send an email outlining your experience and qualifications to jharnetty@ceramics.org.
Sign in to follow this  
Lucille Oka

Ceramics Class

Recommended Posts

Very good Mark. smile.gif

 

Ok newbies, next - Research Sgraffito what does the process entail?

 

Answer this question: Out of the five developement stages of clay, which one is the best to perform the process of Sgraffito? Taking into consideration safety and clarity of images. Why is your answer the best stage?

 

Homework: Make a Sgraffitoed tile.

 

Attention:

More experienced potters feel free to ask your own questions or provide your own mini seminars for the beginners to help them on their clay paths.

Share this post


Link to post
Share on other sites

Answer this question: Out of the five developement stages of

clay, which one is the best to perform the process of Sgraffito? Taking into

consideration safety and clarity of images. Why is your answer the best stage?

 

Homework: Make a Sgraffitoed tile.

 

 

 

 

On my last run I started to use various tools to mark or scratch patterns into the clay. Things I noticed:

 

1. If the clay is less than leather hard the piece became rather messy and difficult to work with. Edges were not as sharp as I intended. Cuts were hard to control.

2. If the clay was a little past leather hard, the tool would not cut smoothly and the edges would fracture leaving rough lines. Cutting motion was jerky and abrupt.

 

So to answer the question I will say leather hard. But within that answer, you have to know the clay body you are working with and when it is most receptive to that kind of treatment.

 

I have rolled out and formed a tile. I think I'll try to scratch out a fish.

 

:)

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

Share this post


Link to post
Share on other sites
Guest JBaymore

To expand.......

 

Using the term "leather hard" seems to imply a "one state" situation. The drying of clay is a continuium from full wet state to completely bone dry. It is such a continuium that it would require hundreds and hundreds of individual terms to "categorize" each possible condition of the clay with a "name".

 

Different effects are achievable from a single process like sgraffito depending on the exact consistency that the slip and clay are at at any given point when you begin to use the process.

 

Technically you can do the scraffito technique on freshly applied wet slip on totally wet clay. It will have a particular character and require a specific way of handling.

 

The idea is to explore and learn the various characteristics throughout that continuium from full wet to full dry so that you can select the correct consistency for the desired effect.

 

best,

 

....................john

Share this post


Link to post
Share on other sites

 

 

On my last run I started to use various tools to mark or scratch patterns into the clay. Things I noticed:

 

1. If the clay is less than leather hard the piece became rather messy and difficult to work with. Edges were not as sharp as I intended. Cuts were hard to control.

2. If the clay was a little past leather hard, the tool would not cut smoothly and the edges would fracture leaving rough lines. Cutting motion was jerky and abrupt.

 

So to answer the question I will say leather hard. But within that answer, you have to know the clay body you are working with and when it is most receptive to that kind of treatment.

 

I have rolled out and formed a tile. I think I'll try to scratch out a fish.

 

smile.gif

 

 

Very good Mark.

I have used 'out of ink' ball point pins, pencils, and a wood stylus (usually comes in a larger wood tool set). I also thought about using a lace making crochet hook haven't done this yet. Leather hard is the best clay stage for me when I want to make angled shapes and lines just like in linocut as a matter of fact the lino cut gouges seem a perfect idea to try as well.

 

If you like your tile and want to install it, place ridges (keys) on the back so that the mastic will adhere better. Who knows maybe you can do a whole school of fish; all types maybe tropical and colorful. You can allow the sgraffitoed lines to create cells or islands to apply color in an on the claypieces.

 

 

Next lesson: Sprigging

 

Define Sprigging.

How can you use it in your work? Can you combine both in one project, Sgraffitto and Sprigging? How about making angel fish?

 

 

 

 

 

 

 

 

 

 

 

 

Share this post


Link to post
Share on other sites

To expand.......

 

Using the term "leather hard" seems to imply a "one state" situation. The drying of clay is a continuium from full wet state to completely bone dry. It is such a continuium that it would require hundreds and hundreds of individual terms to "categorize" each possible condition of the clay with a "name".

 

Different effects are achievable from a single process like sgraffito depending on the exact consistency that the slip and clay are at at any given point when you begin to use the process.

 

Technically you can do the scraffito technique on freshly applied wet slip on totally wet clay. It will have a particular character and require a specific way of handling.

 

The idea is to explore and learn the various characteristics throughout that continuium from full wet to full dry so that you can select the correct consistency for the desired effect.

 

best,

 

....................john

 

 

Going along with this expansion of the state between wet, and leather hard, one of my favorite working times is the "cheese hard" state where the clay will support itself, yet still gives.

 

Often when doing sgraffito where I want clean lines, and edges in dry clay I will use a flexible shaft attached to my dremel with a small fine bit. A little dustier for sure, but much faster, and more fluid. Just don't use too hard or you'll end up with pierced designs. When thinking sgraffito, I also enjoy the opposite technique-Mishima which is also quite stunning when done well.

Share this post


Link to post
Share on other sites

After I coated the tile with a Cobalt slip, I allowed it to slowly dry, testing the clay every day to see if it was ready.

 

I traced a fish on the tile today and then scratched around the design.

 

There is some clean up to do as it finishes drying and I will fire the tile this next weekend.

 

gallery_14105_497_124699.jpg

 

 

:)

Share this post


Link to post
Share on other sites

You do understand that the clay doesn't have to be dry in order to do sgraffito? And it is safer when dampened there is not so much dust. If you are going to do anymore of this method in the dry stage be sure to use a respirator and goggles.

 

To me cobalt is the most beautiful of all the ceramic colorants; it is my favorite. But it does 'spit' while firing in the kiln; I don't mind it. However it doesn't discriminate. The 'spit' lands anywhere so be careful that it doesn't 'spit' on your elements it maybe a good idea to cover the tile with a larger vessel, (use as a saggar) and place upside down and over the tile.

 

Define-saggar

Share this post


Link to post
Share on other sites

Define-saggar

 

 

How funny. I was just reading up on the use of saggars for reduction atmospheres in an electric kiln. B)

Something I will definitely try in the future. I need to buy/design/build one or two saggars for bottom shelf.

 

 

As far as the tile goes, I had it in a plastic bag drying VERY slowly. It was damp for sure and carved quite nicely.

 

:)

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.