jpclay    0

So, yesterday afternoon the power went out while the kiln was bisque firing. I saw the temp when it was over 1600, on the way to ^06. I see today the ^07 has not moved, but I think it probably stopped at about ^08, so I think I can adjust to that. My question is about the clay gases releasing, because the vent stopped when the kiln stopped. The kiln was closed and unvented until early this morning when I was able to restart the vent. Do you think there is a problem with the clay not being vented on the decline temps. Any thoughts? Thank you!

 

Julia Paul

juliapaul.com

Share this post


Link to post
Share on other sites
jpclay    0

The power outage was widespread. Maybe re-fire on faster schedule since it is basically already cooked.

 

Julia Paul

juliapaul.com

Share this post


Link to post
Share on other sites
jpclay    0

With further reading, I see that carbonaceous materials burn out between 500°F–1450°, which leads me to believe that if the pieces are hard enough, the impurities should be burned out and the clay should be ok for glazing.

 

Julia Paul

juliapaul.com

Share this post


Link to post
Share on other sites
Mark C.    1,800

you will be fine-my kiln has no vent and I bisque to 08-no worries

Glaze it up and move on.

Mark

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×