No. Not an issue or problem. Suggest, as a general practice, putting a shelf supported on 1/2 inch posts to serve as bottom. That gives you some space underneath for air/heat circulation. Plus, avoids wear on the kiln floor.

 

 

Good! Also, I've taken this kiln off its rusty old factory issue stand and put it on a heavy duty steel roller dolly. Is this a bad idea?

 

post-13873-135004792605_thumb.jpg

 

post-13873-135004792605_thumb.jpg

Share this post


Link to post
Share on other sites

No. Not an issue or problem. Suggest, as a general practice, putting a shelf supported on 1/2 inch posts to serve as bottom. That gives you some space underneath for air/heat circulation. Plus, avoids wear on the kiln floor.

 

 

Good! Also, I've taken this kiln off its rusty old factory issue stand and put it on a heavy duty steel roller dolly. Is this a bad idea?

 

post-13873-135004792605_thumb.jpg

 

 

 

I would put a kiln shelf between the kiln and the dolly, so the entire bottom has support.

Share this post


Link to post
Share on other sites
Guest JBaymore

Did you check that the top surface of that roller dolly was preciely flat before placing the kiln upon it? If not, then uneven forces on the relatively weak brickwork could have stressed the IFB. Did the cracks show up right after you put it on the dolly?

 

When you stilt the shelves, if you leave that layout on the dolly the same, make sure that the tri-post system you aer using lines up with the three "arms" that are actually supporting the floor. That will keep the withght of the load wells supported instead of relying on the strength of the IFB.

 

That IFB is already being internally thermally "stressed" a bit by being hot on one face and cold on the other over only a distance of 21/2 inches. No sense in adding to the working load.

 

best,

 

.........................john

Share this post


Link to post
Share on other sites

Thanks. I'm starting to think I should just go back to the Skutt stand. With those cracks in the bottom, I wonder if I shouldn't build a firebrick on concrete board 'table' to put on the Skutt stand and the kiln on top of that. I have little space in my shop, so the wheeled dolly (which I had sitting around) seemed perfect. But burning down my house is the risk for the benefit of a little comfort.

 

R

 

 

 

Share this post


Link to post
Share on other sites

I just had this conversation with Skutt a couple weeks ago. They said that it is normal to get fine cracks in the lower slab.

 

As long as the cracks are not going all the way through you should be fine.

 

My kiln is sitting on the factory stand with the Envirovent.

Share this post


Link to post
Share on other sites

If it's not impolite, I'll jump on this thread with a similar question. I am a self-taught potter that has never fired. I recently moved from Oregon back home to Costa Rica, and took an electric kiln with me (it was tested before I shipped it, and passed with plying colors). During the move the metal legs buckled and folded, resulting in some decent cracks in the bottom of the kiln. more than hairline, see the attached pictures.

 

someone recommended using a kiln-repair paste on those bottom cracks, so I had a friend bring some down, but haven't had a chance to use it or test the kiln yet.

My question to you guys, is for tips for a Newbie, on how to baby my kiln to compensate for those cracks. Being in Costa Rica, I can't easily order specialized items, and I can't easily replace that kiln, I need it to last me many years.

 

I will need to come up with a different base since the metal one is busted. I had never considered that the base needed to be perfectly level. what other things should I consider for the base support? I'll need to MacGyver it, and I had originally thought that I could sit the kiln directly on some cement blocks. bad idea?

 

thankfully I brought some extra kiln shelves with me, so I have both full and half shelves. should I just plop one on the bottom of the kiln? should I sit one under the kiln to help distribute the load?

 

thank you all for the amazing resource, this is incredible support.

post-15820-13504603523_thumb.jpg

post-15820-1350460684_thumb.jpg

post-15820-13504603523_thumb.jpg

post-15820-1350460684_thumb.jpg

Share this post


Link to post
Share on other sites

The kiln repair paste should be fine for the major cracks. As the kiln heats, the bricks will expand, so I'd only fill the large ones. I'd sit a full shelf on short posts (1/2 inch) on the bottom -- again, to give some space for air flow during firings. A course or two of bricks can be used as a base; just make sure they are level and have a surface large enough to set the kiln on -- you don't want edges hanging over the sides of the brick base.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.