Porcelain Slip Formula?

Recommended Posts

I am trying to find a recipe for cone 10 Porcelain slip so I can dip fiber art in them for firing. I came across one from a classmate but she made one so long ago. I had a hard time understanding her explaining the recipe. I copied her recipe and now asking you guys if anyone with experience would tell me if this recipe is correct or not. I wrote down exactly what I saw on her paper but I don't understand some parts of it. I am very new at mixing glazes and slips. Forgive me for any spelling errors. Corrections are appreciated!

 

 

Mix first:

 

Barium Carbonate 1/2 oz

 

Soda Ash 1 oz

 

Water 5 gallons

 

Sodium Silicate 2.5 fl oz

 

 

 

Dilute 50/50 with water

 

 

 

Then:

 

25% Super Standard

 

25% Grolleg

 

2% OM4 Ball Clay

 

28% Minspar or G200

 

20% Silica

 

___________________

 

100%

 

 

 

Additives:

 

Gumplast 1 pint

 

Darvan 1 tsp - small like eye dropper

 

 

 

Makes 100 lbs slip

 

 

I hope you understand I do not want to ruin the kiln or accidentally destroy other people's work in the kiln should this slip fail and make a mess. :/ Thanks in advance for your feedback!

 

@deaf258

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×