I am making some ^05 earthenware sculptures that have potentially fragile appendages and joints. (I'll eventually be using cold finishes on the outside.) Would glazing the inside improve their strength?

Share this post


Link to post
Share on other sites

I think I'd ad fiber to the clay rather than count on a glass coating a few mm thick. Glaze is not really a structural element.it is a very thin coating. Maybe it would be better than nothing, but you could run into problems of surface tension with only one side (inside) having glaze on it.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.