Pink Glaze

Recommended Posts

to start you use tin in the base and chrome as the colorant. Go to Clayart archives, MCG and also Digital fire website has a good experiments description. If you read that, you should be able to formulate a pink glaze to your clay and temperature range. I have seen chrome reds as low as ^09 and pinks as high as ^10.

Share this post


Link to post
Share on other sites

hi guys

i heard that we make pink color glaze whit chromium.

who knows how and what should do?

 

 

or - type "chrome tin pink" and "chrome tin red" into google search engine.

 

-h-

 

 

 

Share this post


Link to post
Share on other sites

chrome tin pink or red is one of the fun things possible in cone 6 electric or oxidation - one classic recipe is:

>Chrome /tin cone 6 (red/burgundy)

>Gerstley Borate 21

>Neph sy 16

>Kaolin 11

>whiting 20

>Silica 32

>

>Tin 5

>Chrome ox. .15 (yes point15)

>ron can you recalculate without GB or with sub

the tin of 5.0 and chrome of 0.15 is typical

h a n s e n

 

hi guys

i heard that we make pink color glaze whit chromium.

who knows how and what should do?

 

 

or - type "chrome tin pink" and "chrome tin red" into google search engine.

 

-h-

 

 

 

 

 

 

 

Share this post


Link to post
Share on other sites

p.s. gillespie borate is a workable substitute for gerstley borate

 

chrome tin pink or red is one of the fun things possible in cone 6 electric or oxidation - one classic recipe is:

 

 

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.