I have recently started making molds of carved cylinders and cups. What is the recommended thickness of the plaster mold? (The thickness from the outer wall of the original to the outer edge of the plaster.)

 

Also what is the best cone 10 clay to use for slip, or does someone have a formula they wouldn't mind sharing, for casting? I am looking for something with very little sand, but is cost effective. I have been using Soldate 60 because I have a huge supply of it, but I am not really happy with the roughness of the soldate 60 slip.

 

Thanks in advance

Brian

Share this post


Link to post
Share on other sites
Lucille Oka    16

I have recently started making molds of carved cylinders and cups. What is the recommended thickness of the plaster mold? (The thickness from the outer wall of the original to the outer edge of the plaster.)

 

Brian

 

 

 

Figure on 1 1/2"- 2" thick all around,

-Not so thick that it takes a long time for the mold to dry after you release the casting.

-And not so thin that the mold will saturate with water.

Share this post


Link to post
Share on other sites
perkolator    54

i always shoot for close to 2". gives nice thickness to absorb and not get saturated quick, and not so thick that it's overly heavy. as for casting slip, I cannot comment since I prefer to buy pre-made slip these days. there are plenty of recipes around, but sounds more like you're looking to modify a wet clay body vs start from scratch so I can't comment other than I know it's been done many times.

Share this post


Link to post
Share on other sites
Elmoclayman    0

i always shoot for close to 2". gives nice thickness to absorb and not get saturated quick, and not so thick that it's overly heavy. as for casting slip, I cannot comment since I prefer to buy pre-made slip these days. there are plenty of recipes around, but sounds more like you're looking to modify a wet clay body vs start from scratch so I can't comment other than I know it's been done many times.

 

 

Thanks for the advice. I have made a total of 5 molds so far and have found that 2" seems to work the best.

Share this post


Link to post
Share on other sites
BeckyH    42

If you plan to reuse the molds often and for a long time, a heavier mold will last longer. However, they do need more time to dry between pourings. If the mold is too light, it saturates, as already mentioned, and that leads to crumbling and leakage.

Good luck with your plaster work!

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×