Posted 07 October 2012 - 12:28 PM

What is the specific effect that the artists are trying to achieve using the immersion technique?

Raku Water Immersion


Looks risky to me.
Mark
Fast Hawk Pottery


^5-6 Ox
1227 Skutt

#2 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,120 posts
  • LocationWilton, NH USA

Posted 07 October 2012 - 01:04 PM

Maruku-san, gomen nasai, demo kore wa rakuyaki ja nai, hikidashigoro ga desu.

Mark.... sorry but that is not raku ware, it is Hikidashikuro (Black Seto).

The name translates into about "fire withdrawal black".


Slightly different technique.

In THIS case the water quenching causes the glaze to have sort of a pebbly dry-ish surface and it also causes the clay body to be filled with micro-fractures. This causes the body to lose its hard-fired "ring" factor. Many Chajin (Tea Masters) feel that vitrious stonewares have a harsh sound when the matcha (powdered green tea) is wisked when compared to the teaware "standardbearer"... low fired porous raku wares.

I sometimes do this process in my noborigama. If you look through the photos here ( https://www.facebook...=1&l=7e7b7e21fc ) you'll see a few shots. They are about 1/2 way down the photos. And yeah... it is risky.



best,

.............john

John Baymore
Professor of Ceramics; New Hampshire Insitute of Art

Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#3 Mark McCombs

Mark McCombs

    Advanced Member

  • Members
  • PipPipPip
  • 123 posts
  • LocationSW Washington

Posted 07 October 2012 - 02:19 PM

Mark.... sorry but that is not raku ware, it is Hikidashikuro (Black Seto).

The name translates into about "fire withdrawal black".




No need to be sorry, John. :) I thought I saw the word Raku in one of the translations. Ooops. :rolleyes:


Thank you very much for the explanation. B)

I would love to give that a try some day.
Mark
Fast Hawk Pottery


^5-6 Ox
1227 Skutt

#4 Idaho Potter

Idaho Potter

    Learning all the time

  • Members
  • PipPipPip
  • 403 posts
  • LocationBoise, Idaho

Posted 07 October 2012 - 03:46 PM

I actually water quench my pots after raku firing in a propane kiln, and smoking (post fire reduction)--especially if using a glaze with copper carbonate. Exposure to the air after the reduction causes the glaze to oxidise and lose all the beautiful copper flashes you've achieved in the reduction. Water quenching "sets" the color. I only water quench when using raku clay because it is manufactured to withstand the abrupt thermal changes inherent in this type of firing/reduction. If I use a cone 6 stoneware, I allow the pots to totally cool down in the smoke pot. Using raku clay my losses are less than 10%, stoneware can occasionally rise as high as 40% if not handled carefully.

Shirley

#5 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,120 posts
  • LocationWilton, NH USA

Posted 07 October 2012 - 04:05 PM

Mark,

Afterthought......... I likely should have also noted up there that it is often referred to as "Setoguro" ("Black from Seto").

Think of it as "cone 9 American raku", but no post firing reduction. You can use a gas or electric kiln, not just wood fired. You can air cool them or water quench them .

The claybody MATTERS ;) .



best,

...............john

John Baymore
Professor of Ceramics; New Hampshire Insitute of Art

Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#6 Benzine

Benzine

    Socratic Potter

  • Members
  • PipPipPip
  • 2,400 posts
  • LocationThe Hawkeye State

Posted 07 October 2012 - 07:59 PM

I actually water quench my pots after raku firing in a propane kiln, and smoking (post fire reduction)--especially if using a glaze with copper carbonate. Exposure to the air after the reduction causes the glaze to oxidise and lose all the beautiful copper flashes you've achieved in the reduction. Water quenching "sets" the color. I only water quench when using raku clay because it is manufactured to withstand the abrupt thermal changes inherent in this type of firing/reduction. If I use a cone 6 stoneware, I allow the pots to totally cool down in the smoke pot. Using raku clay my losses are less than 10%, stoneware can occasionally rise as high as 40% if not handled carefully.

Shirley


I too have quenched my wares post reduction. And they definitely ended up with some nice copper effects.