First firing what should we do?10vs6

Recommended Posts

I am a high school ceramics teacher just started at my current school which happends to have a small cantanary arch kiln that has never been fired was built about 10 years ago. I am about to get it hooked up and checked out and really considering 6 reduction. I fire my on work to 6 and my thought is that most of thoes glazes would melt and work in reduction. I also think economically its better and I really dont want to be sitting at school waiting for 10 to drop while my family eats dinner. My questions are would firing schedual be the same I do a body reduction around 08 and would keep in light reduction till 6. Do most oxidation glazes work in reduction. Does anyone have a good cheap base glaze for cone six reduction. Anything else you might want to add about 6 reduction vs. 10 in a classroom setting would be a big help.

Thanks Jpeel

Share this post


Link to post
Share on other sites

[see susan greenleaf's work. she was at the Torpedo Factory in alexandria, virginia for years. probably still is. she gave our guild a wonderful workshop on cone 6 reduction. her pots are spectacular.

Share this post


Link to post
Share on other sites

sounds like you kinda answered your own question with your comments on making your time and fuel consumption more efficient. recently, the trend for schools seems to be a preference to head in the low-fire to ^6 range, although the die-hard stoneware people will always argue that ^10 is preferred. both have their place, just depends on what you're doing. i know a few teachers who do both, but more biased to the ^6 for time savings, etc. and save the ^10 for just a few times a year or for their porcelains, etc.

 

yes, many glazes will work in either ox/red firings, but you'll have to test both ways to really know since there are literally thousands of possible glazes. if you've got some ^6 glazes you are familiar with, stick them in and see what the outcome is. there is a decent article floating around regarding proven ^6 oxy/red glazes that you can pull some recipes from. otherwise, surf the net and you'll find many more. as for your question about "base glaze" do you mean a commercial base glaze or an inexpensive base glaze to make and do different color-ways? i'd say the latter really depends on what materials you have access to currently.

 

for firing, you can take pretty much the same approach you would for your ^10 red and start your reduction around 1700*-ish/^08. to me, the only difference really is when you shut the kiln down.

 

hope this helps! good luck!

Share this post


Link to post
Share on other sites

I fired Cone 6 reduction starting in the 1980s and believe in your situation it would be beneficial for you to do the same. You save roughly 50% in fuel and you also save time. Going to Cone 6 still produces a vitrified Cone 6 body and glazes look like stoneware temperatures. I have several of my tried and true Cone 6 glazes in Michael Baliey's Oriental Glazes book including celadon, copper red, tenmoku, Ohata Red, etc. John Britt published quite a few in 2008 in CM.

I would not mix cone 6 and. Cone 10 in a class room environment. Just pick one and stick with it.

Marcia

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×