I've been using Standard 182, which I like. I might be able to get Laguna clay more locally now, but not Standard, so I'm wondering if anyone has suggestions for a Laguna clay that is similar to 182. I've used #65 and like it for throwing, but it doesn't hold up well with handbuilding; I've used #66, which is better for handbuilding, but I don't like the sand in it for throwing. Any other suggestions would be appreciated!

#2 Lucille Oka

Lucille Oka

    Advanced Member

  • Members
  • PipPipPip
  • 756 posts
  • LocationCalifornia

Posted 07 September 2012 - 06:41 PM

I tried to send you the Laguna clay charts but unfortunately for some reason the post would not go through and was lost. So I recommend going to the Laguna website and look at the clays and see the charts for yourself. Laguna breaks them down to Eastern and Western available clays. They also offer for a small price sample packages of their clays for testing.
John 3:16
"For God so loved the world that He gave His only begotten Son, that whosoever believeth in Him should not perish but have everlasting life".




0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users