yedrow Posted August 22, 2012 Report Share Posted August 22, 2012 I'm sticking handles on these in this video. The clay is real soft so it is whipping at the ends. Other than that it went pretty well. Joel. Link to comment Share on other sites More sharing options...
Denice Posted August 22, 2012 Report Share Posted August 22, 2012 Good video I had forgotten the old pulling off the pot technique. You have refined it and make it easier and faster to do, thank you for the refresher course. Denice Link to comment Share on other sites More sharing options...
LilyT Posted August 22, 2012 Report Share Posted August 22, 2012 thanks! Link to comment Share on other sites More sharing options...
muddylane Posted August 22, 2012 Report Share Posted August 22, 2012 thanks for video..i have commented elsewhere on your lovely handles...just one complaint..I find the music distracting. Am I just old and grumpy? Link to comment Share on other sites More sharing options...
Mark McCombs Posted August 23, 2012 Report Share Posted August 23, 2012 Again, thank you for the vid. Love the music. Link to comment Share on other sites More sharing options...
Mossyrock Posted August 23, 2012 Report Share Posted August 23, 2012 You make it look so easy! Thanks. Link to comment Share on other sites More sharing options...
Juli Long Posted August 24, 2012 Report Share Posted August 24, 2012 I tried some today. Practice makes perfect, and I have a long way to go. Its those little indentions on the sides that I so love. Thanks for finally sharing. I had been waiting. juli Link to comment Share on other sites More sharing options...
yedrow Posted August 24, 2012 Author Report Share Posted August 24, 2012 No probs. Hope those examples help a little. I personally believe that a mug is made by the handle and the handle is made by the negative space. Joel. Link to comment Share on other sites More sharing options...
kathi Posted August 24, 2012 Report Share Posted August 24, 2012 What video are you guys talking about? Kathi Link to comment Share on other sites More sharing options...