Tomorrow is my birthday. Yes, I know it is Friday the 13th! I guess I have to say it is a good luck day since I am turning 59.O.K. Pick yourself up off the floor. I am not using a walker yet. StIll teaching high school art-26 years, and still making pots-35+ years.
Anyway, here are the two glazes. The active ingredient is bone ash, which is a flux and causes the glaze to be a beautiful buttery white.

Tom Roberts Gloss White
Potash spar 20
Whiting 11
Talc 11
E.P.K. 17
Flint 20
Alumina Hydrate 4
Zirco. Pax 6
Bone Ash 5
OM4 Ball clay 6
Total 100

Pete Pinnell's CIA
FRITT 7
Spodumene 15
Neph Sy 10
Syth. Bone Ash 11
Talc 20
EPK 13
Flint 24
Total 100

The second glaze is from Clay Times,Vol II Number 2 [March/April, 2005
Pete suggests adding copper carb in increments of 1%,3%,5%,7%, and 9%.Some beautiful greens result.
These glazes are for cone 9/10 reduction.
Try some colourants and let me know your results.

Gifts gratefully declined for tomorrow.[my birthday,remember]
Tom Roberts, a.k.a. TJR.

#2 yedrow

yedrow

    Advanced Member

  • Members
  • PipPipPip
  • 405 posts

Posted 12 July 2012 - 11:36 PM

Happy birthday!

#3 OffCenter

OffCenter

    Advanced Member

  • Members
  • PipPipPip
  • 1,372 posts

Posted 12 July 2012 - 11:40 PM

Happy B-day. Thanks for the present!

Jim
E pur si muove.

"But it does move," said Galileo under his breath.

#4 scoobydoozie

scoobydoozie

    Advanced Member

  • Members
  • PipPipPip
  • 130 posts
  • LocationClearwater, FL

Posted 13 July 2012 - 07:17 AM

Have a wonderful day! You're only as old as you feel. And... what a great idea to gift to others on your day! Thanks bunches! Posted Image



#5 LilyT

LilyT

    Advanced Member

  • Members
  • PipPipPip
  • 137 posts
  • LocationCalifornia

Posted 13 July 2012 - 09:42 AM

Happy Birthday!
hope your day is spent doing things you like. and thank
you for the present, how lovely and unexpected!

-Lily

#6 Pam S

Pam S

    Advanced Member

  • Members
  • PipPipPip
  • 162 posts
  • LocationDurham, NC

Posted 14 July 2012 - 12:03 AM

Happy birthday (belated)! Thanks for the birthday gift!

"Saving just one dog won't change the world, but it surely will change the world for that one dog."


#7 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,223 posts
  • LocationWilton, NH USA

Posted 15 July 2012 - 11:50 AM

Happy Birthday.

John Baymore
Adjunct Professor of Ceramics; New Hampshire Insitute of Art

Former Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#8 Juli Long

Juli Long

    La Paloma Texas Pottery

  • Members
  • PipPipPip
  • 124 posts
  • Locationtexas

Posted 15 July 2012 - 02:08 PM

Happy birthday, happy late birthday. Nothing like stretching out a birthday for a couple of days.
juli

La Paloma Texas Pottery, Juli Long


#9 SmartsyArtsy

SmartsyArtsy

    Chris Seminara

  • Members
  • PipPipPip
  • 182 posts
  • LocationPNW

Posted 31 July 2012 - 01:05 AM

Belated HAPPY BIRTHDAY TJR!


After 55 it is "legal" and expected that you celebrate 1 week for every year over 55, so you've got 2 more weeks.Posted Image




0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users