Sodium silicatate substitute?

Recommended Posts

Essaily    0

If someone needs are large amount of sodium silicate / magic water

I wondered if Sugar Soap is a safe substitute to use instead of Terra Sigillata?

 

I checked out the ingredients in Selley's Sugar Soap powder and it has the exact ingredients

as the Magic Water terra sigillata recipe I discovered on the Ceramics Arts Daily forum.

 

Neutral salts 60% -

Sodium carbonate -30%

Sodium metasilicate,

pentahydrate -10%

 

Other ingredients determined

not to be hazardous

 

thanks!