Firing gemstones, CZ's etc.

Recommended Posts

Fuad    0

Hi everyone,

 

Has anyone ever fired gemstones (semi-precious or low grade precious) into their work?

 

I was thinking that natural stones might have inclusions that might cause the gem to explode. So that brings me to my next idea - using man made synthetic stones. Would that work?

 

Does anyone know what cone these stones can withstand and still adhere to the glaze?

 

I'm not opposed to the idea of the stones melting and creating interesting effects... I just dont want big black blobs all over my work.

 

Thanks!

Share this post


Link to post
Share on other sites
trina    20

Hi there,

 

 

There are lots of natural red garnets where I live. I find them from time to time, i have tried to fire them, Low fire 1000C, they don't explode but they do turn black. The heat must change them in some way as polishing ect doesn't change them back. I have seen some artists firing stones with silver clay or those type of products at around 700C, haven't tried it myself so don't know for sure how it works. T

Share this post


Link to post
Share on other sites
Amy Waller    7

Here's a link to a forum thread that has some useful information.

 

There's a link to a chart about firing gemstones in that thread, but it doesn't seem to be active. Here's a link to another chart with information about firing gemstones with precious metal clay.

 

Good luck!

Share this post


Link to post
Share on other sites
Antoinette    0

Since the 70's I' ve fired beach sand with pebbles up to about 1/4" using clear glaze to place the sand/pebbles at low fire cone 04 and cone 6 and have never had issues of explosions, crazing or cracking. Actually the firing burns off the impurities/oxidation on the pebbles making whatever color of the pebbles more brilliant. I've gotten my sand/pebble mixture from New England beaches so the composition is primarily black, pink, and white granite.

 

To your point, based on my successes to date, I just recently tried firing semi- precious stones I got at a rock mineral store in AZ as well as petrified wood pieces - not so good results! At cone 6 placed using clear glaze, I got the results in the thread provided in the first response. Since the gems used were silica-based crystal structure, they all turned white! No explosions,crazing or cracking occurred though. So after a discussion with an engineer who works in the coatings business, I was going to try again, this time with a raku firing- lower temp. and very short firing. Again, in reading the threads, this might work...

Share this post


Link to post
Share on other sites
INYA    4

Since the 70's I' ve fired beach sand with pebbles up to about 1/4" using clear glaze to place the sand/pebbles at low fire cone 04 and cone 6 and have never had issues of explosions, crazing or cracking. Actually the firing burns off the impurities/oxidation on the pebbles making whatever color of the pebbles more brilliant. I've gotten my sand/pebble mixture from New England beaches so the composition is primarily black, pink, and white granite.

 

To your point, based on my successes to date, I just recently tried firing semi- precious stones I got at a rock mineral store in AZ as well as petrified wood pieces - not so good results! At cone 6 placed using clear glaze, I got the results in the thread provided in the first response. Since the gems used were silica-based crystal structure, they all turned white! No explosions,crazing or cracking occurred though. So after a discussion with an engineer who works in the coatings business, I was going to try again, this time with a raku firing- lower temp. and very short firing. Again, in reading the threads, this might work...

 

 

 

That sounds really interesting!

Do you have a picture maybe?

Did you spray the glaze?

Thanks!

Share this post


Link to post
Share on other sites
Fuad    0

This sounds very cool Antoinette!

 

I've heard about stones turning opaque and white - and it's not something I'm against happening - but are they more delicate? do they crumble? Do they look just plain ugly?

 

I would love to see some pics of your successes and attempts!

 

Since the 70's I' ve fired beach sand with pebbles up to about 1/4" using clear glaze to place the sand/pebbles at low fire cone 04 and cone 6 and have never had issues of explosions, crazing or cracking. Actually the firing burns off the impurities/oxidation on the pebbles making whatever color of the pebbles more brilliant. I've gotten my sand/pebble mixture from New England beaches so the composition is primarily black, pink, and white granite.

 

To your point, based on my successes to date, I just recently tried firing semi- precious stones I got at a rock mineral store in AZ as well as petrified wood pieces - not so good results! At cone 6 placed using clear glaze, I got the results in the thread provided in the first response. Since the gems used were silica-based crystal structure, they all turned white! No explosions,crazing or cracking occurred though. So after a discussion with an engineer who works in the coatings business, I was going to try again, this time with a raku firing- lower temp. and very short firing. Again, in reading the threads, this might work...

 

Share this post


Link to post
Share on other sites
Lucille Oka    16

There are lots of places to get gemstones, tumbled stones, geodes and pure ores. One place in Arizona I think the name is 'T-Rocks' or 'All In Vein' I am not sure of the name it is near Carl's Jr at 1451 West Main Street in Quartzsite, AZ.

There are semi-precious stone stores in the mall in Tempe, and in stores in Scottsdale. You can also get them at "Beads Galore" in Tempe, AZ.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×