I would like to glaze fire to 05 some portions of bisque fired work and then smoke fire them to get all the non-glazed parts black. How will the glazed parts respond to the smoke firing process? I'll experiment, of course, but if anyone has experience with smoke firing something that has glaze on it, I'd love to hear.

#2 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,069 posts
  • LocationRaleigh, NC

Posted 14 June 2010 - 10:30 AM

I have done it ... You risk some breakage just as you would any re firing but mine mostly came out fine.
I have even fired glazes to cone 6 then raku fired after.

Chris Campbell

Contemporary Fine Colored Porcelain
www.ccpottery.com

 

TRY ... FAIL ... LEARN ... REPEAT

" ... If a sufficient number of people are different, no one has to be normal"
Fredrick Bachman





0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users