Posted 30 April 2012 - 11:56 PM

I asked a while ago for a recipe for white and clear glaze. Clay is earthenware white, temp is 1080C



Any ideas ?





Thanks

#2 bciskepottery

bciskepottery

    Advanced Member

  • Moderators
  • 2,672 posts
  • LocationNorthern Virginia

Posted 01 May 2012 - 06:08 AM

Clear Glaze, Cone 06

Silica, 2%
Ferro Frit 3134, 89.5%
Kaolin, 8.5%
Bentonite, add 2%