Jump to content


Photo

Clear Glaze - White Glaze


  • Please log in to reply
3 replies to this topic

#1 Raku

Raku

    Member

  • Members
  • PipPip
  • 16 posts
  • LocationPerth Western Australia

Posted 27 April 2012 - 08:00 PM

Anyone got a reliable EARTHENWARE recipe for a Clear Glaze and a White Glaze. Both for functional wares.



Thanks

#2 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,058 posts
  • LocationRaleigh, NC

Posted 27 April 2012 - 09:28 PM

You are asking a simple question that is incredibly tough to answer ... Closest accurate answer is ... it all depends.
What is your clay body? What temp will you be firing it to? What kind of kiln ... Oxidation or reduction?

Chris Campbell

Contemporary Fine Colored Porcelain
www.ccpottery.com

 

TRY ... FAIL ... LEARN ... REPEAT

" ... If a sufficient number of people are different, no one has to be normal"
Fredrick Bachman


#3 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,128 posts
  • LocationRed Lodge, Montana

Posted 28 April 2012 - 05:47 AM

If you knew the temperature (cone) and the clay body ("earthenware" covers a wide range) you could just google that. The question is too vague to answer.


Marcia

Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#4 Raku

Raku

    Member

  • Members
  • PipPip
  • 16 posts
  • LocationPerth Western Australia

Posted 28 April 2012 - 06:53 PM

You are asking a simple question that is incredibly tough to answer ... Closest accurate answer is ... it all depends.
What is your clay body? What temp will you be firing it to? What kind of kiln ... Oxidation or reduction?


White Earthenware, 1080C electric