I have a bunch of type N thermocouple wire. I suspect the answer is no, but can I use this for a type K thermocouple? If not, anyone need some type N thermocouple wire, lol.

#2 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,124 posts
  • LocationWilton, NH USA

Posted 24 April 2012 - 09:43 AM

Nope... it will skew the readings.

best,

...............john

John Baymore
Professor of Ceramics; New Hampshire Insitute of Art

Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#3 yedrow

yedrow

    Advanced Member

  • Members
  • PipPipPip
  • 405 posts

Posted 24 April 2012 - 12:34 PM

**snaps his fingers and mumbles something better left a mumble**




0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users